A&A Products  -   Aanraku Glass_Studios   -   American_Glass_Supply  -  Anything_in_Stained_Glass  -   Armstrong Glass Company  -  Artisan_Dichroic  -   Blue_Fire_Molds   -   Bullseye_Glass   -   COE90.com  -  Curious_Glass_Shop  -   Delphi_Glass  -   Dichro_Depot  -   Dichroic_and_More   -    Ed_Hoy's_International  -  Evenheat_Kilns  -  Hang_Your_Glass  -   His_Glassworks  -  Hollander_Fusing_Center  -  Hot_Glass_Houston   -   Kiln_Frog   -   Lincoln_Distributors  -   Nartique_Glass  -   Olympic_Kilns  -  Paragon_Kilns  -      Skutt_Kilns   -   Slumpy's   -   System_96   -   TMS_Studios   -   Uroboros_Glass   -   Warm_Glass_UK   -   Wasser_Glass

Tutorial  Links & Resources Contemporary Fused Glass book Glass Gallery Warm Glass Bulletin Board Warm Glass Courses Warm Tips

 

WARM GLASS GALLERY

 

 
  • Red and Black Cake Plate with adhesive attached legs.

  • The legs, which are 9mm thick, were slumped and then attached with Loctite UV glue with activator.  To ensure solid attachment the piece was heated to 200F for 45 minutes to fully cure the glue.

  • 16" round x 6.75" high

Click here to send an email to Stacey Street.

Click here to return to the list of artists.

This art  is protected by copyright and may not be reproduced and or copied without the express permission of the owner, Stacey Street.

 

All works depicted on this website are protected by copyright and should not be reproduced

and/or copied without the express permission of the respective artists.

 

 

Click here to see a list of all the artists represented in the online Warm Glass Gallery.

 

Return to top About Warm Glass

Privacy Policy

 
 
Warm Glass

Warm Glass

2575 Old Glory Road

Suite 700

Clemmons, NC  27012   USA

Visit the Warm Glass Gallery & Studio for classes, supplies, and more

 

 

Copyright 1999 - 2008 by M. Bradley Walker.  All rights reserved.

Designed, implemented, and published by Four Corners International, Inc.