Search found 29 matches
- Sat Oct 19, 2013 6:57 pm
- Forum: Techniques and Tools
- Topic: Printer questions for decals
- Replies: 16
- Views: 18858
Re: Printer questions for decals
From what I understand from the search, the iron oxide content of the laser printer toners is what produces sepia results. But I still am having trouble finding out if it's possible to print a decal that's still black after firing from home. **ETA: Screen printing, from what I'm understanding from t...
- Sat Oct 19, 2013 8:44 am
- Forum: Techniques and Tools
- Topic: Printer questions for decals
- Replies: 16
- Views: 18858
Printer questions for decals
I'm ready to purchase a printer for making my own decals, BUT I'm still not sure which one to buy. I mostly make dichro jewelry in a jen ken kiln and I also have a microwave kiln. 1) I would REALLY like to be able to print off decals that will fire BLACK and not SEPIA. Is this possible? 2) I've read...
- Thu Jun 27, 2013 7:14 pm
- Forum: Newcomer Forum
- Topic: Questions for first kiln use
- Replies: 9
- Views: 14037
Re: Questions for first kiln use
When something does come out quite right, do you typically try to first increase hold times, or increase temperature? I used the guide on that link that was posted above. My mold was similar but had more "slots" in it. They weren't quite "right". Also, can I re-fire these in the ...
- Fri Jun 21, 2013 4:55 pm
- Forum: Newcomer Forum
- Topic: Questions for first kiln use
- Replies: 9
- Views: 14037
Re: Questions for first kiln use
When something does come out quite right, do you typically try to first increase hold times, or increase temperature? I used the guide on that link that was posted above. My mold was similar but had more "slots" in it. They weren't quite "right". Also, can I re-fire these in the ...
- Mon Jun 17, 2013 10:00 am
- Forum: Newcomer Forum
- Topic: Questions for first kiln use
- Replies: 9
- Views: 14037
Re: Questions for first kiln use
Thanks Brad! Is glass separator the same thing as kiln wash, and is primer also the same thing?
- Sun Jun 16, 2013 8:36 pm
- Forum: Newcomer Forum
- Topic: Questions for first kiln use
- Replies: 9
- Views: 14037
Questions for first kiln use
I got a Jen-Ken AF3P Fuse Box 6/4.5 Flex kiln from Kiln Frog. My first kiln. I started out using a Fuseworks microwave kiln. It came with a little bit of "high fire kiln wash" and it says to apply to kiln shelf (which I already knew to do), and to the kiln bottom. Is this correct? Why woul...
- Sun Jun 02, 2013 10:45 pm
- Forum: Newcomer Forum
- Topic: Tips on how to avoid this mistake?
- Replies: 5
- Views: 6241
Re: Tips on how to avoid this mistake?
Thanks for the tip Brad, I will try your tips!
- Sun Jun 02, 2013 10:16 pm
- Forum: Newcomer Forum
- Topic: Tips on how to avoid this mistake?
- Replies: 5
- Views: 6241
Re: Tips on how to avoid this mistake?
Thanks for your reply. I do get a lot of good ones, that's for sure. I got the microwave kiln because this is my first time ever making anything like this before and I wanted to be sure I'd enjoy it. Well, I have a "real" kiln ordered but it won't be here for a few weeks probably!
- Sun Jun 02, 2013 5:16 pm
- Forum: Newcomer Forum
- Topic: Tips on how to avoid this mistake?
- Replies: 5
- Views: 6241
Tips on how to avoid this mistake?
I've been fusing small cabochons for earrings in my microwave kiln. Some come out pretty much perfect, but sometimes they don't. I am wondering if the problem lies in the size of the glass pieces, or the placement of the pieces prior to fusing? I have a hard time getting uniform shapes and sizes. Fo...