Search found 50 matches

by BobbieMatus
Wed Nov 15, 2017 8:54 am
Forum: Techniques and Tools
Topic: Spectrum from Mexico
Replies: 1
Views: 5600

Spectrum from Mexico

Has anyone used spectrum coming from Oceanside (mexico). I'm wondering about quality
by BobbieMatus
Wed Mar 29, 2017 2:54 pm
Forum: Techniques and Tools
Topic: Spectrum 96
Replies: 2
Views: 7608

Spectrum 96

Has anyone heard any news about 96 glass being available and when. I also heard there maybe someone else besides oceanside
by BobbieMatus
Tue Feb 14, 2017 12:40 pm
Forum: Techniques and Tools
Topic: ceramic molds
Replies: 7
Views: 16921

Re: ceramic molds

thanks everyone
by BobbieMatus
Mon Feb 13, 2017 2:08 pm
Forum: Techniques and Tools
Topic: ceramic molds
Replies: 7
Views: 16921

ceramic molds

Is there a way to clean off the accumulated kiln wash on ceramic molds. Every time I slump pieces of kiln wash get embedded on my piece.
by BobbieMatus
Sun May 22, 2016 4:07 pm
Forum: Techniques and Tools
Topic: SPECTRUM GLASS CLOSING DOWN
Replies: 29
Views: 143902

Re: SPECTRUM GLASS CLOSING DOWN

It is a sad day for me to see Spectrum go. I just bought all the spectrum I could afford hopefully to get me through my season here in Fl going from Oct to March. I got an email from Uroboros stating that they will produce 96 however, they will not be making any Baroque or smooth glass. Can't imagin...
by BobbieMatus
Fri Feb 21, 2014 4:04 pm
Forum: Techniques and Tools
Topic: Kilns
Replies: 24
Views: 99074

Re: Kilns

yes it is the original controller. So the real question is if I buy a new kiln which one. I would like to here from everyone which kilns they like the best.
by BobbieMatus
Fri Feb 21, 2014 9:04 am
Forum: Techniques and Tools
Topic: Kilns
Replies: 24
Views: 99074

Re: Kilns

Most of the rust is by the peep hole so I'm thinking it's better to keep that closed and just crack the lid an inch. That's what I'm trying now. New top element is in, pain in the neck to do, some chipping now on top. should I use kiln cement? Kiln still needs to be rewired and I quess we will have ...
by BobbieMatus
Thu Feb 20, 2014 1:33 pm
Forum: Techniques and Tools
Topic: Kilns
Replies: 24
Views: 99074

Re: Kilns

I use thin fire so I'm keeping the lid open just a little to 1000 degrees should I keep the peep hole open as well or close it? Is this crashing?? How does everyone vent their kiln. I tried doing the kiln wash but doing shows alsmost every week-end and constantly working made thin fire a must for me...
by BobbieMatus
Thu Feb 20, 2014 10:42 am
Forum: Techniques and Tools
Topic: Kilns
Replies: 24
Views: 99074

Re: Kilns

I think it rusted out because I was venting through the peep hole. Mike at JenKen told me to crack the top open and vent to 1000 degrees. How are all of you venting.
by BobbieMatus
Wed Feb 19, 2014 4:53 pm
Forum: Techniques and Tools
Topic: Kilns
Replies: 24
Views: 99074

Re: Kilns

kiln wash is not an option for me as I fire everyday. didn't know about stretching the elements
by BobbieMatus
Wed Feb 19, 2014 1:33 pm
Forum: Techniques and Tools
Topic: Kilns
Replies: 24
Views: 99074

Kilns

I have a 28 inch JenKen which is now completely rusted out, husband says it needs to be rewired and he hates the quality of it. I fire everyday, kiln is about 12 years old . I replaced the lid two years ago.I burn out elements a lot and my husband replaces them cursing as he does it. My question is ...
by BobbieMatus
Fri Aug 24, 2012 3:39 pm
Forum: Techniques and Tools
Topic: turquoise opal 96 question
Replies: 11
Views: 23580

Re: turquoise opal 96 question

sounds like the most possibilty
by BobbieMatus
Fri Aug 24, 2012 11:41 am
Forum: Techniques and Tools
Topic: turquoise opal 96 question
Replies: 11
Views: 23580

Re: turquoise opal 96 question

didn't use any glue on body of cat. I use super glue and used it only on the legs. I emailed spectrum and their first response was glue. Spectrum has asked me to mail them a piece of the glass.
by BobbieMatus
Fri Aug 24, 2012 8:27 am
Forum: Techniques and Tools
Topic: turquoise opal 96 question
Replies: 11
Views: 23580

Re: turquoise opal 96 question

there is only the bubble between the clear and the turquoise. there was nothing on the glass, no label
by BobbieMatus
Thu Aug 23, 2012 8:46 pm
Forum: Techniques and Tools
Topic: turquoise opal 96 question
Replies: 11
Views: 23580

Re: turquoise opal 96 question

glue was used only on legs and tail not on body of cat
by BobbieMatus
Thu Aug 23, 2012 4:08 pm
Forum: Techniques and Tools
Topic: turquoise opal 96 question
Replies: 11
Views: 23580

turquoise opal 96 question

I recently fired a piece of turquoise opal 96 with clear 96 on top and there was a metal looking blob plus a bubble after the firing. Has this happened to anyone? firing schedule
400 to 1220 hold 20 min
400 to 1450 hold 10 min
full to 950 hold 30 min
by BobbieMatus
Mon Dec 08, 2003 9:46 am
Forum: Techniques and Tools
Topic: Finally got to meet one of you
Replies: 6
Views: 14481

Miss the mountains

Been to Utah once when the kids were little and we did a cross country trip with a motorhome. Truly beautiful place. I'm originally from New York and do miss the mountains and especially miss rocks. Florida has no real rocks just that coral stuff. Before I moved to Fl. I lived in Rockland county. Mo...
by BobbieMatus
Thu Dec 04, 2003 9:09 am
Forum: Techniques and Tools
Topic: Finally got to meet one of you
Replies: 6
Views: 14481

How, nice. I always say, sooner or later everyone comes to Florida.
Bobbie
by BobbieMatus
Wed Dec 03, 2003 11:35 am
Forum: Techniques and Tools
Topic: Finally got to meet one of you
Replies: 6
Views: 14481

Florida

I'm in the North end of Palm Beach Gardens almost Jupiter. Pretty far from the Pan Handle.
Bobbie
by BobbieMatus
Wed Dec 03, 2003 11:30 am
Forum: Business Topics
Topic: What's selling? Survey Says!
Replies: 52
Views: 94940

Florida selling

Just wanted to give my two cents worth. I'm selling only items under $40.00, mostly wine bottles and my small lady stuff. Haven't sold any large pieces or even mid range pieces. My work ranges from $20.00 to $2200.00. Added the inexpensive fused pieces this year and it has helped since the large pie...