Vonon, the lines are 6mm wide Bullseye stripes, on the edge. Forgot to mention the clear glass is on top of the black one, so we see the stripes from top and side.
Thank you so much for your kind comments.
Search found 2 matches
- Tue Aug 26, 2014 4:08 pm
- Forum: Photos and Stuff
- Topic: Black plate with a red puddles window
- Replies: 12
- Views: 17332
- Sat Aug 23, 2014 4:50 pm
- Forum: Photos and Stuff
- Topic: Black plate with a red puddles window
- Replies: 12
- Views: 17332
Black plate with a red puddles window
Here is my first post, a 9 mm Bullseye glass plate : 3 mm black, 6 mm clear, white and red stripes and a window made of puddles (thanks to Paul Tarlow's puddles tutorial). It was fun to make it, I hope you'll enjoy the pictures. I'd like to thank you all for the advice, information and discussions o...