Re: fibre paper channel question
Thank you very much for the very helpful reply! I tried it and I did have a little cold working to do but not as much as with it run straight through. Great suggestion!
- Tue Oct 29, 2013 10:55 am
- Forum: Jewelry Making
- Topic: fibre paper channel question
- Replies: 2
- Views: 7598
fibre paper channel question
Hello, I have been experimenting with creating a channel in my glass pendants instead of the glue on bail option. The only issue I am having is that the glass pulls at the fibre paper during firing which leaves me with sharp edges at the opening on the finished piece. Short of cold working and re-fi...