Re: Molds to large for kiln?
Thank you for the good advice. I think I will contact Colour de Verre for the definitive word, but think I may have jumped the gun with grand plans before I even set up the kiln. Among other things, I bought some Kaiser Lee board to use as a kiln shell to avoid the mess with shelf papers. I think th...
- Fri Dec 27, 2013 12:20 pm
- Forum: Newcomer Forum
- Topic: Molds to large for kiln?
- Replies: 9
- Views: 15035
Molds to large for kiln?
I just bought, but have not yet received, a Jen Ken AF3P ProFusion 16 fiber kiln with inside dimension of: 16" x 16" x 5". There is no shelf so need to use fiber paper on the bottom, kaiser lee board, or lava cloth. Anticipating the kind of projects I had in mind, I bought a round 10 ...