The OHAUS Triple Beam Balance is a solid and time tested standard for up to 2610g. Additional Counter weights increase the 610g amount that can be weighed. The scales are extremely accurate and will out live most of us.
kittyboy
Search found 3 matches
- Mon Jun 09, 2014 7:11 pm
- Forum: Newcomer Forum
- Topic: Searching for a scale accurate to .1g
- Replies: 10
- Views: 12393
- Sun Jun 08, 2014 5:20 pm
- Forum: Kiln Casting
- Topic: Dental plaster
- Replies: 17
- Views: 31192
Re: Dental plaster
Thanks Kittyboy, this is interesting. I have seen suggestions to replace silica flour with alumina hydrate but this is the first time I have seen alumina oxide suggested. Do you have any information comparing the two alumina compounds in terms of their application for glass casting molds - ie. refr...
- Sat Jun 07, 2014 9:14 pm
- Forum: Kiln Casting
- Topic: Dental plaster
- Replies: 17
- Views: 31192
Re: Dental plaster
Edit Mode.