I think their may need to be a wider range to sign up for something like this. Perhaps a couple months in place of a couple weeks would help?
- Fri Jan 30, 2015 7:54 pm
- Forum: Newcomer Forum
- Topic: Cutting, devit spray, and other questions
- Replies: 12
- Views: 18379
Re: Cutting, devit spray, and other questions
Yeah I've been capping in clear so it's very evident. I'll try other colors.
- Fri Jan 30, 2015 6:32 pm
- Forum: Newcomer Forum
- Topic: Cutting, devit spray, and other questions
- Replies: 12
- Views: 18379
Re: Cutting, devit spray, and other questions
This is bullseye thinfire paper but I'm not very happy with it. I have 50 sheets of useless 20 inch wide paper then... wonderful. I suppose I'll learn to use kiln wash. This paper also shrinks an incredible amount, I suppose this is normal but for the price I think it's absurd. I'll vent the kiln an...
- Fri Jan 30, 2015 3:05 pm
- Forum: Newcomer Forum
- Topic: Cutting, devit spray, and other questions
- Replies: 12
- Views: 18379
Re: Cutting, devit spray, and other questions
Two layers 3mm: one designed, one clear coat on the top. I only grind when I need to take off a slant from the occasional break on a 3mm non fused piece. But I tried cutting a 6mm piece 12 inches wide and it was a holy disaster. I bought a 7 inch tile saw to tackle these issues. On a different note,...
- Wed Jan 28, 2015 5:38 pm
- Forum: Newcomer Forum
- Topic: Cutting, devit spray, and other questions
- Replies: 12
- Views: 18379
Cutting, devit spray, and other questions
20150110_113212.jpg 1.I make large (12 inch) plates, every time I score with a wheel and try to break it, the break doesn't go cleanly and it ends up ruining the piece or I have to grind for 30 minutes to make it look clean. Could I use a tile saw on a 12 inch plate while keeping the work area from...