Help - troubleshoot cracked glass
I built three panels approximately 19 inches by 24 inches and approximately .25" to 3/8ths inch thick. The firing schedule I used is: 150 500 20 150 800 20 150 1100 20 50 1250 10 9999 1470 20 9999 960 4 hours 100 700 1 hour I cold worked the panels. the client installed the panels into a window...