oh, got it. yeah, I think 1600 is best for bottle and window glass.Judd wrote:Jim said Cone 015 for BE glass. Window and bottle glasses need more heat.
Search found 7 matches
- Tue Oct 31, 2017 12:50 am
- Forum: Kiln Casting
- Topic: bottle glass frit - firing schedule
- Replies: 13
- Views: 23098
Re: bottle glass frit - firing schedule
- Mon Oct 30, 2017 2:37 am
- Forum: Kiln Casting
- Topic: bottle glass frit - firing schedule
- Replies: 13
- Views: 23098
Re: bottle glass frit - firing schedule
oh, that's 1456F. you mean even for soda lime glass?jim simmons wrote:for BE frit I wouldn't go above cone 015
The other Jim
at 1456F it wasn't melted well for bottle glass.
- Mon Oct 30, 2017 2:35 am
- Forum: Kiln Casting
- Topic: bottle glass frit - firing schedule
- Replies: 13
- Views: 23098
Re: bottle glass frit - firing schedule
I make my own kiln wash. I use 20% EP Kaolin, 80% Alumina Hydrate. Even with that, I have had sticking at Cone 05. I know when they make African Powder beads, they have a lot of sticking. They wash the beads in a sand/water slurry. Hi Jodd, Thank you for your comments. Ok, I might need to down more...
- Thu Oct 26, 2017 8:18 pm
- Forum: Kiln Casting
- Topic: bottle glass frit - firing schedule
- Replies: 13
- Views: 23098
Re: bottle glass frit - firing schedule
For fusing compatible art frit, make sure that your mold is prepped. I use ZYP coating from colour de verre. You can also use BE kiln wash. Then after you put in the frit, either/and/or, mound it in the center of the mold with the sides a little way FROM the mold. This will allow the frit to CLIMB ...
- Thu Oct 26, 2017 5:05 pm
- Forum: Kiln Casting
- Topic: bottle glass frit - firing schedule
- Replies: 13
- Views: 23098
Re: bottle glass frit - firing schedule
Are you wanting to make something like the African Bottle Beads? If so, you should crush your glass until its powder. If you're expecting your frit to smooth out like fusing glass, that will never happen unless you hit really high temps - like 2000 Fahrenheit. At least, that has been my experience....
- Wed Oct 25, 2017 1:13 pm
- Forum: Kiln Casting
- Topic: bottle glass frit - firing schedule
- Replies: 13
- Views: 23098
Re: bottle glass frit - firing schedule
Thank you! Yeah, I think it's really hard to make the casting beads.
I will look up more:)
I will look up more:)
- Tue Oct 24, 2017 12:51 am
- Forum: Kiln Casting
- Topic: bottle glass frit - firing schedule
- Replies: 13
- Views: 23098
bottle glass frit - firing schedule
Hi all! I am new to glasswork(lampwork, fusing glass). I try to use the bottle glass to make beads. From the lampworking, I got nice beads with using bottle glass, but I am still struggling with bottle frit casting. I made frits from bottle glass and tested them on the molds with the several firing ...