Hi all I’m new at this. Would love advice about the ratio to combine two glass enamel powders to achieve a different colour. I want a deep dark red and am looking at Thompson’s ‘Victoria’ and ‘Flame Red’
I am however finding it hard to find somewhere to buy these two colours. I’m in Australia.
Search found 1 match
- Mon Oct 24, 2022 6:01 am
- Forum: Newcomer Forum
- Topic: Ratio for combining two glass enamels
- Replies: 4
- Views: 20386