Right before you had posted the picture, I had realized you had not, and was awaiting it, as you never disappoint with your Christmas suncatchers. Really do enjoy them.
Thanks
Mike
Search found 20 matches
- Sun Dec 30, 2012 12:08 am
- Forum: Photos and Stuff
- Topic: 2012 Xmas Suncatcher
- Replies: 13
- Views: 13468
- Sun Apr 18, 2004 6:43 pm
- Forum: Techniques and Tools
- Topic: sink slumping delimma
- Replies: 4
- Views: 5120
- Sun Apr 18, 2004 10:07 am
- Forum: Techniques and Tools
- Topic: sink slumping delimma
- Replies: 4
- Views: 5120
- Fri Apr 16, 2004 11:31 am
- Forum: Techniques and Tools
- Topic: sink slumping delimma
- Replies: 4
- Views: 5120
sink slumping delimma
I recently took Patty Grays sink class. The mold we recieved is 19 in ID across, 9 3/4 deep. I do not have a kiln big enough to do the slumping. The local glass blower has offered the use of hers if either one will work. Options are, annealing kiln, side elements three sides, big enough to hold alea...
- Wed Apr 14, 2004 10:27 pm
- Forum: Techniques and Tools
- Topic: stainless steel question
- Replies: 21
- Views: 35675
- Wed Apr 14, 2004 9:58 am
- Forum: Techniques and Tools
- Topic: stainless steel question
- Replies: 21
- Views: 35675
- Wed Apr 14, 2004 9:26 am
- Forum: Techniques and Tools
- Topic: stainless steel question
- Replies: 21
- Views: 35675
stainless steel question
I have a couple of SS rings, that I hope to use as drop out rings. Question is, can I? or will their be expansion/contraction problems. Will the ring (18 ga.) warp, will I be able to get the glass out of the ring. Thanks Mike
- Fri Apr 09, 2004 2:36 pm
- Forum: Techniques and Tools
- Topic: Bas relief slump
- Replies: 3
- Views: 3616
- Fri Apr 09, 2004 2:05 pm
- Forum: Techniques and Tools
- Topic: Bas relief slump
- Replies: 3
- Views: 3616
Bas relief slump
Couldn't find in the archive, so here's the question. Float glass circle 10in., 1/4in. glass. Using fiber paper design cut out. When slumping into a SS bowl, will I lose much of the design element. Thanks Mike
- Fri Apr 09, 2004 9:10 am
- Forum: Techniques and Tools
- Topic: BIG Adhesive Question
- Replies: 13
- Views: 15276
I use UV6800. It a silicone based adhesive, doesn't yellow. I have used it and haven't had a loose piece yet. Then again have only used it for 3 years. Comes in a 10oz. caulk gun tube, and a 4oz squeeze tube. I get it from Adhesive Plus (972) 422-2180. They are out of Texas, apparently they manufact...
- Sun Mar 28, 2004 12:50 pm
- Forum: Techniques and Tools
- Topic: Paragon Kiln help and question on 3 key controller
- Replies: 7
- Views: 7400
- Sun Mar 28, 2004 12:14 pm
- Forum: Techniques and Tools
- Topic: Paragon Kiln help and question on 3 key controller
- Replies: 7
- Views: 7400
Which 3 key controller is it? Paragon sold 2. In the past it was the Bartlett board, now it is the Orton. I am a Paragon Certified repair person (That certificate and 10¢ still will not buy me a cup of coffee), but have the person drop me an e-mail with what the code is and then I can get them wha...
- Thu Mar 18, 2004 8:34 pm
- Forum: Techniques and Tools
- Topic: stainless steel
- Replies: 5
- Views: 6221
- Thu Mar 18, 2004 7:52 pm
- Forum: Techniques and Tools
- Topic: stainless steel
- Replies: 5
- Views: 6221
stainless steel
Have aquired some 18 gauge stainless steel for rings. Has been cut into 3/4in. strips. Even though it will be lined with paper. should the SS, be prefired. Thanks. Mike
- Mon Mar 08, 2004 9:30 am
- Forum: Photos and Stuff
- Topic: [color=red]Patty Gray's sink class at Studio B in Seattle -
- Replies: 4
- Views: 6428
- Sat Feb 14, 2004 12:22 am
- Forum: Techniques and Tools
- Topic: Jen-Ken Kiln question
- Replies: 12
- Views: 13162
Re: Jen-Ken Kiln question
Hi all, After much reading on this board, I've finally decided to by a Jen-Ken kiln. I'm getting it directly from them so that I can just go pick it up and save on shipping. I thought I knew what I wanted untill they asked me if I wanted to get the kiln with or without the viewing window. I have an...
- Mon Feb 09, 2004 4:44 pm
- Forum: Photos and Stuff
- Topic: A little splash of color
- Replies: 30
- Views: 33308
- Mon Feb 09, 2004 9:09 am
- Forum: Photos and Stuff
- Topic: A little splash of color
- Replies: 30
- Views: 33308
- Wed Jan 21, 2004 11:45 pm
- Forum: Techniques and Tools
- Topic: Another good place for kiln formed glass classes
- Replies: 10
- Views: 8673
- Fri Nov 28, 2003 10:35 pm
- Forum: Techniques and Tools
- Topic: Need help 2
- Replies: 2
- Views: 3671
Need help 2
New to the board, and need loads of help. To start with, after reviewing the archieve, didn't find the answer I was looking for. If I have a wrought iron shape, and put my glass in it, with out some sort of kiln wash to the sides or fire paper, will the glass stick to the sides, and during to coolin...