I took it to 1700, then i combed, then held at 1700 for 30 min. I was a
little afraid that i would comb too hard and go thru glass into shelf.
John
Search found 11 matches
- Wed Mar 10, 2004 12:48 am
- Forum: Photos and Stuff
- Topic: First Combing Try
- Replies: 2
- Views: 4679
- Tue Mar 09, 2004 11:56 pm
- Forum: Photos and Stuff
- Topic: First Combing Try
- Replies: 2
- Views: 4679
First Combing Try
My first attempt at combing, i probably didn't move tool around enough, but as i said it's my first attempt. Let me know what you think. The help that i get here makes me want to try new things, and i know that i will only get good advice. Thanks John http://community.webshots.com/photo/124350231/12...
- Sun Mar 07, 2004 12:57 am
- Forum: Photos and Stuff
- Topic: Had to try Potmelt
- Replies: 8
- Views: 9954
- Sun Mar 07, 2004 12:43 am
- Forum: Photos and Stuff
- Topic: Had to try Potmelt
- Replies: 8
- Views: 9954
- Fri Mar 05, 2004 10:00 pm
- Forum: Photos and Stuff
- Topic: Had to try Potmelt
- Replies: 8
- Views: 9954
Had to try Potmelt
After reading and seeing the results of others I too had to try my hand at Potmelts. Don't know if i used too many colors, because they seem too (for the lack of a better word) busy. Had no trouble with the process and left over glass stuck to pot (39 cents at Michaels). When loading should i random...
- Sun Feb 08, 2004 8:27 pm
- Forum: Techniques and Tools
- Topic: what happened to my dollar bill
- Replies: 4
- Views: 5926
- Sat Feb 07, 2004 10:21 pm
- Forum: Techniques and Tools
- Topic: what happened to my dollar bill
- Replies: 4
- Views: 5926
what happened to my dollar bill
Tried the dollar bill between to clear pieces. Came out with big air bubble
a little negative image on back side but that's all. Thought it would look
better that this. Or is this what i am to expect? http://community.webshots.com/photo/116 ... 1706Ykzvsm
Help appreciated.
John
a little negative image on back side but that's all. Thought it would look
better that this. Or is this what i am to expect? http://community.webshots.com/photo/116 ... 1706Ykzvsm
Help appreciated.
John
- Sun Jan 18, 2004 3:06 pm
- Forum: Photos and Stuff
- Topic: Comments on picture frame
- Replies: 6
- Views: 7347
Let's try this http://community.webshots.com/user/joeat515
- Sun Jan 18, 2004 1:32 pm
- Forum: Photos and Stuff
- Topic: Comments on picture frame
- Replies: 6
- Views: 7347
- Sun Jan 18, 2004 12:30 pm
- Forum: Photos and Stuff
- Topic: Comments on picture frame
- Replies: 6
- Views: 7347
Comments on picture frame
New to fusing, am making picture frames for my 3 sons graduation pictures.This is the first one and it came out ok except for hazy look on 2/3rds of clear cap glass. Probably due to cleaning. But am learing so hope i won't make same mistake again. http://community.webshots.com/s/image9/9/15/61/11209...
- Sun Jan 18, 2004 12:18 am
- Forum: Techniques and Tools
- Topic: Hazy look after clear cap
- Replies: 1
- Views: 2400
Hazy look after clear cap
This is my first attempt at fusing, have read books and have been checking out the Bulletin Board Forums. Made a picture frame using Sys 96 glass, it came out ok for my first try. But i thought it would look better capped with clear glass. Fused piece again but about 2/3rds of it came out hazy, the ...