Search found 40 matches

by StaceyG
Thu Jan 30, 2014 2:46 pm
Forum: Techniques and Tools
Topic: sink mold used for hanging light?
Replies: 17
Views: 37649

Re: sink mold used for hanging light?

Curious if you have made this, would love to see a photo. How did you support it when drilling the holes and what type of hardware did you use?
by StaceyG
Wed Dec 18, 2013 3:51 pm
Forum: Techniques and Tools
Topic: Removing glass plug from diamond drill bit
Replies: 25
Views: 65562

Re: Removing glass plug from diamond drill bit

If I cant get the glass out, I put the bit in a vice and then take a nail, and hammer the glass so it breaks up in to tiny pieces that will just fall out.
by StaceyG
Fri Jun 21, 2013 9:08 am
Forum: Photos and Stuff
Topic: And another drop ring vessel
Replies: 11
Views: 31261

Re: And another drop ring vessel

I use a flat lap grinder to smooth and polish the edges. It was a big investment but well worth it. Also helped to grind off some kiln wash that got stuck on the bottom of a flat piece.
by StaceyG
Thu May 30, 2013 2:44 pm
Forum: Techniques and Tools
Topic: Silver leaf/foil
Replies: 9
Views: 22131

Re: Silver leaf/foil

Can you fuse it uncapped? It shouldn't turn yellow that way.
by StaceyG
Thu May 30, 2013 2:42 pm
Forum: Photos and Stuff
Topic: Chili hot pepper
Replies: 11
Views: 19942

Re: Chili hot pepper

Really nice work!
by StaceyG
Tue May 28, 2013 12:45 pm
Forum: Photos and Stuff
Topic: And another drop ring vessel
Replies: 11
Views: 31261

Re: And another drop ring vessel

I remove them very carefully with a tile saw.
by StaceyG
Fri May 24, 2013 8:58 am
Forum: Photos and Stuff
Topic: And another drop ring vessel
Replies: 11
Views: 31261

Re: And another drop ring vessel

Oh my gosh Tracy, you are absolutely right! You just made my day. Putting in an order now! :D
by StaceyG
Thu May 23, 2013 8:59 am
Forum: Photos and Stuff
Topic: And another drop ring vessel
Replies: 11
Views: 31261

Re: And another drop ring vessel

They both used scraps I had from Bullseye limited sheet glass, that used French Vanilla and light turquoise blue. I think I have enough left to make 1-2 more vases, but after that I am out of luck, since this was a "limited edition" glass.
by StaceyG
Thu May 23, 2013 7:40 am
Forum: Photos and Stuff
Topic: And another drop ring vessel
Replies: 11
Views: 31261

And another drop ring vessel

This one used more opaque glass and dropped a little deeper than the other one. The lip came off a lot more easily on this one, thanks goodness. Less coldwork to do!
by StaceyG
Thu May 23, 2013 5:16 am
Forum: Photos and Stuff
Topic: Drop Ring Vessel
Replies: 9
Views: 21568

Re: Drop Ring Vessel

Its about 5" high.
by StaceyG
Wed May 22, 2013 7:52 pm
Forum: Photos and Stuff
Topic: Drop Ring Vessel
Replies: 9
Views: 21568

Re: Drop Ring Vessel

The hole in the center is about 3".
by StaceyG
Wed May 22, 2013 11:29 am
Forum: Photos and Stuff
Topic: Drop Ring Vessel
Replies: 9
Views: 21568

Drop Ring Vessel

After much trial and error, I have a presentable drop ring vessel. I used 4 layers of glass, and it dropped about 5". 3 layers was sometimes just a little too thin. I like the feel of the heavier vessel with 4 layers, so I think I will stick with that. The colors remind me of the beach, so I am...
by StaceyG
Mon Mar 25, 2013 12:09 pm
Forum: Techniques and Tools
Topic: Arranging glass on shelf
Replies: 16
Views: 30997

Re: Arranging glass on shelf

Do you have a lighttbox? Maybe you can trace the pattern onto the shelf paper using your laser print out.
by StaceyG
Thu Feb 14, 2013 1:51 pm
Forum: Techniques and Tools
Topic: Pearl 22 - lid removal?
Replies: 0
Views: 21228

Pearl 22 - lid removal?

Hi, I am receiving a Paragon Pearl 22 kiln tomorrow. Does anyone know if its possible, or how easy it is (for my mechanically inclined husband) to remove the lid to make it lighter to lift up on to my table? He changed the pneumatic thing in my trunk recently, so I hope these skills might also apply...
by StaceyG
Wed Feb 13, 2013 2:46 pm
Forum: Newcomer Forum
Topic: Draping Problem
Replies: 10
Views: 25300

Re: Draping Problem

Thanks, I will check mine tonight. I know I don't have that "anneal now" button though, that seems VERY handy.
by StaceyG
Wed Feb 13, 2013 2:26 pm
Forum: Newcomer Forum
Topic: Draping Problem
Replies: 10
Views: 25300

Re: Draping Problem

And make sure you peek now and then when you're approaching top temp, so you can move on to annealing when your drape looks like you want it to. This might be a stupid question, but if you have programmed your kiln, how do you move on to the annealing when it looks like you want it to look? Do you ...
by StaceyG
Wed Feb 13, 2013 2:22 pm
Forum: Techniques and Tools
Topic: Cutting rim off drop ring vessel
Replies: 3
Views: 10002

Re: Cutting rim off drop ring vessel

I can imagine its hard to keep it still on the grinder. Thanks for the information. I think this is something I might tackle down the road, since I don't currently have a lap grinder.

Stacey
by StaceyG
Tue Feb 12, 2013 2:41 pm
Forum: Techniques and Tools
Topic: Cutting rim off drop ring vessel
Replies: 3
Views: 10002

Cutting rim off drop ring vessel

What is the best way to cut the rim off a drop ring, so it becomes a "rimless" vase. Any suggestions for best way to cold work that edge, can you successfully use sanding pads, or would I need something like a lap grinder or belt sander?

Stacey
by StaceyG
Tue Feb 12, 2013 2:37 pm
Forum: Techniques and Tools
Topic: Viewing windows in kilns
Replies: 8
Views: 18686

Re: Viewing windows in kilns

I just purchased a new kiln and asked the shop owner the same thing. He said no. Why do you need one? You can just open the kiln to check on glass. he also said they can let air escape, even if ever so slightly.
by StaceyG
Sun Feb 10, 2013 10:24 am
Forum: Techniques and Tools
Topic: Durock-vitrigraph kiln
Replies: 5
Views: 10396

Durock-vitrigraph kiln

Can you use durock as the bottom of a vitrigraph kiln instead of fiber board?