Search found 40 matches
- Thu Jan 30, 2014 2:46 pm
- Forum: Techniques and Tools
- Topic: sink mold used for hanging light?
- Replies: 17
- Views: 21116
Re: sink mold used for hanging light?
Curious if you have made this, would love to see a photo. How did you support it when drilling the holes and what type of hardware did you use?
- Wed Dec 18, 2013 3:51 pm
- Forum: Techniques and Tools
- Topic: Removing glass plug from diamond drill bit
- Replies: 25
- Views: 32894
Re: Removing glass plug from diamond drill bit
If I cant get the glass out, I put the bit in a vice and then take a nail, and hammer the glass so it breaks up in to tiny pieces that will just fall out.
- Fri Jun 21, 2013 9:08 am
- Forum: Photos and Stuff
- Topic: And another drop ring vessel
- Replies: 11
- Views: 17924
Re: And another drop ring vessel
I use a flat lap grinder to smooth and polish the edges. It was a big investment but well worth it. Also helped to grind off some kiln wash that got stuck on the bottom of a flat piece.
- Thu May 30, 2013 2:44 pm
- Forum: Techniques and Tools
- Topic: Silver leaf/foil
- Replies: 9
- Views: 12705
Re: Silver leaf/foil
Can you fuse it uncapped? It shouldn't turn yellow that way.
- Thu May 30, 2013 2:42 pm
- Forum: Photos and Stuff
- Topic: Chili hot pepper
- Replies: 11
- Views: 12390
Re: Chili hot pepper
Really nice work!
- Tue May 28, 2013 12:45 pm
- Forum: Photos and Stuff
- Topic: And another drop ring vessel
- Replies: 11
- Views: 17924
Re: And another drop ring vessel
I remove them very carefully with a tile saw.
- Fri May 24, 2013 8:58 am
- Forum: Photos and Stuff
- Topic: And another drop ring vessel
- Replies: 11
- Views: 17924
Re: And another drop ring vessel
Oh my gosh Tracy, you are absolutely right! You just made my day. Putting in an order now!
- Thu May 23, 2013 8:59 am
- Forum: Photos and Stuff
- Topic: And another drop ring vessel
- Replies: 11
- Views: 17924
Re: And another drop ring vessel
They both used scraps I had from Bullseye limited sheet glass, that used French Vanilla and light turquoise blue. I think I have enough left to make 1-2 more vases, but after that I am out of luck, since this was a "limited edition" glass.
- Thu May 23, 2013 7:40 am
- Forum: Photos and Stuff
- Topic: And another drop ring vessel
- Replies: 11
- Views: 17924
And another drop ring vessel
This one used more opaque glass and dropped a little deeper than the other one. The lip came off a lot more easily on this one, thanks goodness. Less coldwork to do!
- Thu May 23, 2013 5:16 am
- Forum: Photos and Stuff
- Topic: Drop Ring Vessel
- Replies: 9
- Views: 12693
Re: Drop Ring Vessel
Its about 5" high.
- Wed May 22, 2013 7:52 pm
- Forum: Photos and Stuff
- Topic: Drop Ring Vessel
- Replies: 9
- Views: 12693
Re: Drop Ring Vessel
The hole in the center is about 3".
- Wed May 22, 2013 11:29 am
- Forum: Photos and Stuff
- Topic: Drop Ring Vessel
- Replies: 9
- Views: 12693
Drop Ring Vessel
After much trial and error, I have a presentable drop ring vessel. I used 4 layers of glass, and it dropped about 5". 3 layers was sometimes just a little too thin. I like the feel of the heavier vessel with 4 layers, so I think I will stick with that. The colors remind me of the beach, so I am...
- Mon Mar 25, 2013 12:09 pm
- Forum: Techniques and Tools
- Topic: Arranging glass on shelf
- Replies: 16
- Views: 16060
Re: Arranging glass on shelf
Do you have a lighttbox? Maybe you can trace the pattern onto the shelf paper using your laser print out.
- Thu Feb 14, 2013 1:51 pm
- Forum: Techniques and Tools
- Topic: Pearl 22 - lid removal?
- Replies: 0
- Views: 17289
Pearl 22 - lid removal?
Hi, I am receiving a Paragon Pearl 22 kiln tomorrow. Does anyone know if its possible, or how easy it is (for my mechanically inclined husband) to remove the lid to make it lighter to lift up on to my table? He changed the pneumatic thing in my trunk recently, so I hope these skills might also apply...
- Wed Feb 13, 2013 2:46 pm
- Forum: Newcomer Forum
- Topic: Draping Problem
- Replies: 10
- Views: 12125
Re: Draping Problem
Thanks, I will check mine tonight. I know I don't have that "anneal now" button though, that seems VERY handy.
- Wed Feb 13, 2013 2:26 pm
- Forum: Newcomer Forum
- Topic: Draping Problem
- Replies: 10
- Views: 12125
Re: Draping Problem
And make sure you peek now and then when you're approaching top temp, so you can move on to annealing when your drape looks like you want it to. This might be a stupid question, but if you have programmed your kiln, how do you move on to the annealing when it looks like you want it to look? Do you ...
- Wed Feb 13, 2013 2:22 pm
- Forum: Techniques and Tools
- Topic: Cutting rim off drop ring vessel
- Replies: 3
- Views: 6379
Re: Cutting rim off drop ring vessel
I can imagine its hard to keep it still on the grinder. Thanks for the information. I think this is something I might tackle down the road, since I don't currently have a lap grinder.
Stacey
Stacey
- Tue Feb 12, 2013 2:41 pm
- Forum: Techniques and Tools
- Topic: Cutting rim off drop ring vessel
- Replies: 3
- Views: 6379
Cutting rim off drop ring vessel
What is the best way to cut the rim off a drop ring, so it becomes a "rimless" vase. Any suggestions for best way to cold work that edge, can you successfully use sanding pads, or would I need something like a lap grinder or belt sander?
Stacey
Stacey
- Tue Feb 12, 2013 2:37 pm
- Forum: Techniques and Tools
- Topic: Viewing windows in kilns
- Replies: 8
- Views: 10690
Re: Viewing windows in kilns
I just purchased a new kiln and asked the shop owner the same thing. He said no. Why do you need one? You can just open the kiln to check on glass. he also said they can let air escape, even if ever so slightly.
- Sun Feb 10, 2013 10:24 am
- Forum: Techniques and Tools
- Topic: Durock-vitrigraph kiln
- Replies: 5
- Views: 6415
Durock-vitrigraph kiln
Can you use durock as the bottom of a vitrigraph kiln instead of fiber board?