I guess it's too late now, but what if you cast your glass as a single piece with a stem connecting the leaf and flower, then cast the metal in two pieces which you then join around the stem? All pieces would be cast, and joined by soldering; you'd need to work the soldered seam into the design.
Lee
Search found 8 matches
- Thu Apr 01, 2004 5:34 pm
- Forum: Techniques and Tools
- Topic: kiln casting with metal... please help!
- Replies: 50
- Views: 49453
- Thu Apr 01, 2004 5:21 pm
- Forum: Techniques and Tools
- Topic: PMC for glass fusing jewelry
- Replies: 17
- Views: 21164
Re: PMC for glass fusing jewelry
[quote="Terry Ow-Wing"]Does the silver fuming wreck the kiln or do something that makes it not workable for glass? Silver fumes can change the color of some colors of glass (I know Moretti dark ivory is one, not sure of others). It can be a very interesting effect, some beadmakers use it, ...
- Thu Mar 11, 2004 8:42 pm
- Forum: Techniques and Tools
- Topic: francais
- Replies: 15
- Views: 17104
- Sat Mar 06, 2004 10:03 pm
- Forum: Techniques and Tools
- Topic: old glass
- Replies: 2
- Views: 3375
- Sat Mar 06, 2004 9:01 pm
- Forum: Techniques and Tools
- Topic: old glass
- Replies: 2
- Views: 3375
old glass
I made torchwork beads for a while about 10 years ago, then had to pack up everything to move and am finally getting everything out again so I can make beads and learn fusing and slumping. So I've got about 50 glass rods of various colors, and I can't remember :oops: what manufacturer they're from. ...
- Thu Mar 04, 2004 12:36 pm
- Forum: Kiln Casting
- Topic: latex mold Q?s
- Replies: 5
- Views: 8092
- Mon Mar 01, 2004 1:42 pm
- Forum: Kiln Casting
- Topic: Cypress Electrical kiln Model# 9140S
- Replies: 1
- Views: 3541
- Fri Feb 27, 2004 3:29 pm
- Forum: Kiln Casting
- Topic: Cypress Electrical kiln Model# 9140S
- Replies: 1
- Views: 3541
Cypress Electrical kiln Model# 9140S
Hi all,
has anyone heard of a Cypress Electrical Kiln? I've been offered one cheap, but can't find a listing online to see what it's like.
Any help?
thanks
Lee
has anyone heard of a Cypress Electrical Kiln? I've been offered one cheap, but can't find a listing online to see what it's like.
Any help?
thanks
Lee