Search found 29 matches
- Wed May 14, 2003 11:20 am
- Forum: Techniques and Tools
- Topic: fusing
- Replies: 5
- Views: 7018
- Tue Apr 29, 2003 9:24 am
- Forum: Techniques and Tools
- Topic: new to warm glass and having trouble already
- Replies: 5
- Views: 6289
- Fri Apr 25, 2003 11:25 am
- Forum: Kiln Casting
- Topic: "Mixing with the Best" - great reference material!
- Replies: 3
- Views: 7141
"Mixing with the Best" - great reference material!
I just received in the mail yesterday the casting information CD that has been mentioned in a couple of posts recently. I highly recommend it. The CD is called, "Mixing with the Best - Investigation and Comparison of Contemporary Working Methods and Mould Making Materials For Use in the Kiln Fo...
- Tue Apr 15, 2003 4:54 pm
- Forum: Techniques and Tools
- Topic: Pestle and mortar for crushing glass
- Replies: 15
- Views: 22324
Elaine: Try a search in the old archives. Several people have made frit crushers out of old garbage disposal units. Liam has some pictures: http://www.warmglass.com/cgi-bin/wgarchive3.pl?read=77091 Have you seen Brad's how to's? http://www.warmglass.com/making_your_own.htm#FRIT Hope this might help ...
- Sat Apr 05, 2003 11:49 am
- Forum: Photos and Stuff
- Topic: Online Fusing Presentation
- Replies: 14
- Views: 18540
Lisa: That is a very well done presentation. Great pictures and informative text. How long will it stay up on that website? I have been wondering if your pieces with the long sliced pattern bars that you have posted pictures of are the same two layer bases. There doesn't seem to be much spreading fr...
- Tue Apr 01, 2003 10:38 pm
- Forum: Techniques and Tools
- Topic: problems w/ 14" sq mold
- Replies: 6
- Views: 8278
- Tue Apr 01, 2003 10:32 am
- Forum: Techniques and Tools
- Topic: problems w/ 14" sq mold
- Replies: 6
- Views: 8278
Jeri: A couple of suggestions: 1) Make sure the air holes in your mold are not plugged with kiln wash. 2) Depending on the shape of your mold raising it off the shelf with some kiln furniture or pieces of fiber paper will help the air escape. Is the mold sitting on the shelf so that the air holes ar...
- Wed Mar 19, 2003 7:01 pm
- Forum: Techniques and Tools
- Topic: Glass Artist TV Shows
- Replies: 3
- Views: 7074
- Sat Mar 15, 2003 1:14 pm
- Forum: Techniques and Tools
- Topic: Felisatti question
- Replies: 42
- Views: 81578
Candy:
This topic started in a thread further down "Wet grinder question for Doug"
The link to the supplier is:
http://www.granitecitytoolvt.com/specialsales.html
The Felisatti is at the bottom of the page.
Good luck
Jane
This topic started in a thread further down "Wet grinder question for Doug"
The link to the supplier is:
http://www.granitecitytoolvt.com/specialsales.html
The Felisatti is at the bottom of the page.
Good luck
Jane