Re: Mold Mix 6 or 7 ????

Hello Jagboy69 I believe you were asking how to work with Mold Mix 6, so I did some PDF's and video for Zircar so here a link for you . Les
https://www.youtube.com/watch?v=le96sNV_b0Y&t=28s
by twin vision glass
Tue Jul 16, 2019 2:15 pm
Forum: Techniques and Tools
Topic: MM6
Replies: 3
Views: 50

Re: MM6

Hi dear Brad, hope you are well. A while ago some artists were asking about how to work with Mold Mix 6 so I did this video and Zircar has 4 PDF's also to help others to be able to work with this casting material that has been part of my life for 30 years and I have loved working with it and hope ot...
by twin vision glass
Mon Jul 15, 2019 10:45 pm
Forum: Techniques and Tools
Topic: MM6
Replies: 3
Views: 50

MM6

There was a discussion awhile ago about Zircar Luminar MM6 . Many were wanting to know how to use it so I decided to try to help out by working with Zircar and doing a video and some PDF s for them. They have posted the video ( so surprised how older I look :cry: ) but hey it is not about me, it is ...
by twin vision glass
Fri May 17, 2019 4:19 pm
Forum: Kiln Casting
Topic: Mold Mix 6 or 7 ????
Replies: 13
Views: 472

Re: Mold Mix 6 or 7 ????

Zircar Refractory Composites has been so very supportive over the years trying very hard to create items that will work for the glass community. Thomas Hamling Traveled to Pilchuck Glass School during one of our residency's so he could see how MM6 and other products worked for the glass community, a...
by twin vision glass
Thu May 16, 2019 4:13 pm
Forum: Kiln Casting
Topic: Mold Mix 6 or 7 ????
Replies: 13
Views: 472

Re: Mold Mix 6 or 7 ????

You should be able to achieve a beautiful surface on your glass with no splitting of the mold so no cold working . Also Flame working multiple face molds is awesome with MM6 .
phpBDUqHyPM.jpg
phpDvhypMPM.jpg
by twin vision glass
Thu May 16, 2019 4:05 pm
Forum: Kiln Casting
Topic: Mold Mix 6 or 7 ????
Replies: 13
Views: 472

Re: Mold Mix 6 or 7 ????

phpSTqsgPPM.jpg
by twin vision glass
Thu May 16, 2019 4:02 pm
Forum: Kiln Casting
Topic: Mold Mix 6 or 7 ????
Replies: 13
Views: 472

Re: Mold Mix 6 or 7 ????

a one day seminar on Luminar Mold Mix 6 ( which we will video tape so that it can be sold for artists to use if this is something that interests you) Location: Passion For Glass , 1534 17th Ave. SW. , Calgary, AB , Canada ( 587 353 2153 ) Artist : Leslie Rowe-Israelson Date : Saturday , June 22th Ti...
by twin vision glass
Thu May 16, 2019 3:57 pm
Forum: Kiln Casting
Topic: Mold Mix 6 or 7 ????
Replies: 13
Views: 472

Re: Mold Mix 6 or 7 ????

I am trying to get a demonstration of how to create with MM6 and will video tape the seminar . I am working with Brooke at Zircar Refractory Composites ( Thomas Hamling's daughter ) who has invested a great deal of time to get the perfect product for us . The seminar we hope will be held at Passion ...
by twin vision glass
Thu May 02, 2019 11:49 pm
Forum: Techniques and Tools
Topic: BE Dense White (0313) Reaction
Replies: 5
Views: 352

Re: BE Dense White (0313) Reaction

php2N6kUIPM.jpg
phpSTqsgPPM.jpg
phpHQ2J7fPM.jpg
phpHQ2J7fPM.jpg (20.75 KiB) Viewed 310 times
by twin vision glass
Thu May 02, 2019 11:46 pm
Forum: Techniques and Tools
Topic: BE Dense White (0313) Reaction
Replies: 5
Views: 352

Re: BE Dense White (0313) Reaction

You know what gives a fabulous reaction is Robin Egg Blue and French Vanilla. Simply awesome
by twin vision glass
Thu May 02, 2019 11:42 pm
Forum: Kiln Casting
Topic: Mold Mix 6 or 7 ????
Replies: 13
Views: 472

Re: Mold Mix 6 or 7 ????

Here is how the piece should come out if done right. http://www.twinvision.fusedglassartists.com/ The full sized head was cast in MM6 nestled in sand for backing !
by twin vision glass
Thu May 02, 2019 11:40 pm
Forum: Kiln Casting
Topic: Mold Mix 6 or 7 ????
Replies: 13
Views: 472

Re: Mold Mix 6 or 7 ????

wM and L034.jpg I have worked with Mold Mix 6 for years. I like the MM6 as it is not in powder format . What is the shape you are trying to cast . Mold Mix 6 can get very hard if painted on tooo thick. I like it for soft and sensual shapes . But once you get used to using it , you can use it in mos...
by twin vision glass
Fri Apr 26, 2019 2:17 pm
Forum: Photos and Stuff
Topic: The Latest Bowl
Replies: 8
Views: 1894

Re: The Latest Bowl

Late to post as well but send our heart felt hugs and love. Just so tragic . I hope life gets better for you and your amazing inspiring art.
by twin vision glass
Thu Apr 25, 2019 10:10 pm
Forum: Photos and Stuff
Topic: Birds Nest
Replies: 0
Views: 177

Birds Nest

phpifiMEwPM.jpg
phpifiMEwPM.jpg (15.4 KiB) Viewed 177 times
phpDAjQf8PM.jpg
phpBVZL7bAM.jpg
by twin vision glass
Wed Jul 11, 2018 2:45 pm
Forum: Photos and Stuff
Topic: Playing with Color Bars and Vitrigraph
Replies: 4
Views: 1890

Re: Playing with Color Bars and Vitrigraph

phpbpwu4zAM.jpg
phpbpwu4zAM.jpg (50.48 KiB) Viewed 1845 times
by twin vision glass
Sun Jul 08, 2018 9:14 am
Forum: Photos and Stuff
Topic: Playing with Color Bars and Vitrigraph
Replies: 4
Views: 1890

Re: Playing with Color Bars and Vitrigraph

phpZzbPrEPM.jpg
phpZzbPrEPM.jpg (49.27 KiB) Viewed 1882 times
How are you Kevin. Here is the ground being created.
by twin vision glass
Sat Jul 07, 2018 10:05 pm
Forum: Photos and Stuff
Topic: Playing with Color Bars and Vitrigraph
Replies: 4
Views: 1890

Playing with Color Bars and Vitrigraph

I have been having fun slicing and chopping and creating with color bars and vitrigraph.
php2KGdH9PM.jpg
php2KGdH9PM.jpg (52.52 KiB) Viewed 1890 times
phpqmiAuzPM.jpg
phpqmiAuzPM.jpg (46.97 KiB) Viewed 1890 times
by twin vision glass
Sat Jun 16, 2018 9:22 am
Forum: Photos and Stuff
Topic: Getting ready to blow out Color Bar in HOT shop
Replies: 13
Views: 4423

Re: Getting ready to blow out Color Bar in HOT shop

Hi Sharol, It is great to share again with everyone. I tooo have missed posting in Warm Glass.
phphS7OcoPM.jpg
My twin and I are having fun pulling out the slices on the torch as well. It is just so fun to take this beautiful material and manipulate it hot.
by twin vision glass
Mon May 21, 2018 10:49 am
Forum: Photos and Stuff
Topic: Getting ready to blow out Color Bar in HOT shop
Replies: 13
Views: 4423

Re: Getting ready to blow out Color Bar in HOT shop

phpMh3DA6AM.jpg
phpTpcyNaAM.jpg
phpTpcyNaAM.jpg (46.63 KiB) Viewed 4131 times
always fun to go get a nice pic
by twin vision glass
Sat May 12, 2018 8:47 am
Forum: Photos and Stuff
Topic: Getting ready to blow out Color Bar in HOT shop
Replies: 13
Views: 4423

Re: Getting ready to blow out Color Bar in HOT shop

Thank you Ed, I love taking the Bullseye Glass to the hot shop and manipulating it. The large cast glass bars are the best to begin with for me for a more organic look.

Go to advanced search

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com