Search found 560 matches
- Mon Oct 01, 2012 5:41 pm
- Forum: Techniques and Tools
- Topic: Why did my plate break?
- Replies: 11
- Views: 9674
Re: Why did my plate break?
I toooo feel it was too quick and I never go faster than 100 deg. per hour unless tiny pieces. I even go 50 deg. per hour with thick work. Les
- Mon Oct 01, 2012 11:48 am
- Forum: Photos and Stuff
- Topic: Uroboros Residency
- Replies: 44
- Views: 42279
Re: Uroboros Residency
Thankyou so much Oritt, how is your glass going these days. Les
- Sun Sep 30, 2012 7:24 pm
- Forum: Photos and Stuff
- Topic: "WINTERS COMING"
- Replies: 16
- Views: 15422
Re: "WINTERS COMING"
O.K. now I am happy, we just changed the belt on my saw as it was taking so very long through a cut AND WOW!!!!!!!!!!!!!!!!!!!! I am saving hours. I also have 4 new blades coming that I am testing and will keep you all informed on which is my favorite.
Leslie
Leslie
- Sun Sep 30, 2012 2:29 pm
- Forum: Photos and Stuff
- Topic: "WINTERS COMING"
- Replies: 16
- Views: 15422
"WINTERS COMING"
Since the winter is apon us I am inspired to create some new snow mountain scenes. Here are the slices that will be incorporated into the glass panels
- Fri Sep 28, 2012 6:37 pm
- Forum: Newcomer Forum
- Topic: Pattern Bar Slices
- Replies: 3
- Views: 5271
Re: Pattern Bar Slices
Hi! the only parts of the slices that I grind are the parts that have touched the mold or kiln shelf. UNLESS you have used fiber then make sure you grind off all the particles that could make for a scummy join. the glass will not flow as nicely if you have particles exposed. I tooo think the pieces ...
- Fri Sep 28, 2012 2:49 pm
- Forum: Photos and Stuff
- Topic: Uroboros Residency
- Replies: 44
- Views: 42279
Re: Uroboros Residency
http://www.canadahouse.com/dynamic/artw ... rkID=29627 Yeah! it has found a home. Les
- Fri Sep 28, 2012 2:45 pm
- Forum: Photos and Stuff
- Topic: Uroboros Residency
- Replies: 44
- Views: 42279
Re: Uroboros Residency
:oops: Risa and Bob, not only was I exhausted after the residency with border guards and other things making my trip to the U.S. difficult, but at the end it was ALL worth every red and tired face I earned. The owners and the staff go over backwards to make your stay in their studio an"A" ...
- Fri Sep 28, 2012 1:26 pm
- Forum: Techniques and Tools
- Topic: WHY did they break?
- Replies: 19
- Views: 16188
Re: WHY did they break?
http://www.bullseyeglass.com/index.php? ... 1348849519
Not sure if this will help out or not. But pile up sections on the kiln shelf and above and you will get some truly marvelous things happening.
Not sure if this will help out or not. But pile up sections on the kiln shelf and above and you will get some truly marvelous things happening.
- Fri Sep 28, 2012 1:24 pm
- Forum: Techniques and Tools
- Topic: WHY did they break?
- Replies: 19
- Views: 16188
Re: WHY did they break?
Some of my mesh melts are lower and longer. So I will go up: - 100 degrees F. per hour to 1220 - Hold 2 hours - 150 degrees F. to 1480 F. ( if I have dense white in the piece then I will keep it at 1480 for only 15 minutes depending oh the holes) BUT I also have alot of mass and depth to the melts I...
- Fri Sep 28, 2012 1:17 pm
- Forum: Photos and Stuff
- Topic: Uroboros Residency
- Replies: 44
- Views: 42279
Re: Uroboros Residency
It is called " AUTUMN"S FIRST SNOW FALL " and the sky is a bit dramatic but not so much that it takes away from the piece. So thankyou Rosanna, that means alot.
- Fri Sep 28, 2012 12:45 pm
- Forum: Techniques and Tools
- Topic: WHY did they break?
- Replies: 19
- Views: 16188
Re: WHY did they break?
Dear Havi, I am not sure it is wise to take the glass to such high temps. Perhaps contact Bullseye and ask if something else is actually happening to the glass at that temp and changing some coefficients . Just a thought friend. Leslie (can you not achieve the same thing at a lower/ longer temp sche...
- Fri Sep 28, 2012 12:34 pm
- Forum: Photos and Stuff
- Topic: Uroboros Residency
- Replies: 44
- Views: 42279
Re: Uroboros Residency
Thankyou so kindly . I love creating with colour bars as you do get a much more painterly approach, and I am so glad you noticed.
Les
Les
- Fri Sep 28, 2012 1:16 am
- Forum: Photos and Stuff
- Topic: Uroboros Residency
- Replies: 44
- Views: 42279
Re: Uroboros Residency
I was experimenting with a softer sky and I like it . It is not so busy!
- Tue Sep 25, 2012 12:32 pm
- Forum: Techniques and Tools
- Topic: new shop/studio
- Replies: 6
- Views: 6122
Re: new shop/studio
Yes, at the end of October. Have some wonderful artists in the class and can hardly waite to share with them. My only worry is the noise from the sawing process so I might have to moon light to saw up the bars. :-k . The class is at PASSION FOR GLASS and I look forward to it very much. Leslie (p.s. ...
- Tue Sep 25, 2012 11:50 am
- Forum: Techniques and Tools
- Topic: new shop/studio
- Replies: 6
- Views: 6122
Re: new shop/studio
:cry: :-k [-o< Oh if anyone has the patience , you do Rick. Perhaps something completely new will come out of all the new experiments! :D I look soooo forward to seeing your new studio . I myself am waiting patiently for 4 new blades to experiment with to somehow speed up the sawing process AND am p...
- Sun Sep 23, 2012 8:39 pm
- Forum: Photos and Stuff
- Topic: 2012 Pilchuck Glass Auction catalog
- Replies: 13
- Views: 14107
Re: 2012 Pilchuck Glass Auction catalog
Hmmm! not sure why.
- Sat Sep 22, 2012 2:30 pm
- Forum: Photos and Stuff
- Topic: Koi
- Replies: 4
- Views: 5826
Re: Koi
I love to see artists take risks and try new directions with their work. You will never know where it takes you and the swim down the river is truly a new adventure. Hmmm! dinner for someone perhaps. Yum! Leslie
- Fri Sep 21, 2012 11:58 am
- Forum: Techniques and Tools
- Topic: MESH MELT DISASTER
- Replies: 21
- Views: 21015
Re: MESH MELT DISASTER
I think if you had a ceramic kiln shelf that you could saw and use as supports for your wire mesh you would not have had it bend. :cry: Sad when that happens. The design will be alot more swirling when the drop is so far as well. Also do you need to go that hot. I love to go lower longer, taking lon...
- Thu Sep 20, 2012 9:36 pm
- Forum: Photos and Stuff
- Topic: 2012 Pilchuck Glass Auction catalog
- Replies: 13
- Views: 14107
Re: 2012 Pilchuck Glass Auction catalog
http://issuu.com/pilchuckglassschool/docs/pilchuck_catalog__12/81#print I think this is the correct link to my page tooo. Well done Dolores! beautiful piece as always. You cannot see the beads on my donation but my twin and I had alot of fun creating this piece out of Uroboros Glass at our residency...
- Wed Sep 19, 2012 7:57 pm
- Forum: Photos and Stuff
- Topic: Upon the Mere - A New Bowl
- Replies: 20
- Views: 23763
Re: Upon the Mere - A New Bowl
I also love the edge and not the constraints of a border.