Denise, I think the answer lies in the size/importance of the piece. If it's a small piece of jewelry, just clean the surface well, cap it with clear, and fire. Not much lost if it doesn't come out perfectly clean. If, however, it is a significant piece, either in size or cost of materials, or time ...
- Wed Jun 11, 2003 6:55 am
- Forum: Techniques and Tools
- Topic: Slides/photographs of kiln-formed wall sconces wanted
- Replies: 10
- Views: 10192
Slides/photographs of kiln-formed wall sconces wanted
Greetings,
I am researching for an article on kiln-formed wall sconces (or other types of lighting fixtures) I would welcome slides and/or photos - and any information you might want to share. I will, of course, fully credit each contributing artist.
thanks,
judith
I am researching for an article on kiln-formed wall sconces (or other types of lighting fixtures) I would welcome slides and/or photos - and any information you might want to share. I will, of course, fully credit each contributing artist.
thanks,
judith
- Thu May 22, 2003 7:35 am
- Forum: Techniques and Tools
- Topic: Useful New Class!!! (A review)
- Replies: 4
- Views: 5538
Sounds like a great class, you guys. I want to take one for a change. It'll be yours or one of Bob's. and I'd like to join Lani in her appraisal of your studio. From what we've seen, it is by far the best equipped, best staffed, and best run private teaching studio in North America. Way to go. Broc...
- Mon May 19, 2003 12:19 pm
- Forum: Techniques and Tools
- Topic: Useful New Class!!! (A review)
- Replies: 4
- Views: 5538
- Thu May 15, 2003 7:48 am
- Forum: Business Topics
- Topic: Nearest airport to Vitrum Studio
- Replies: 4
- Views: 7784
Re: Nearest airport to Vitrum Studio
Hi, I didn't know whether to post this question on Spab or Business. I am registered for Bob Leatherbarrow's Powder and Frit Class at Vitrum in Laurel/Beltway, MD this month. I've been looking for cheap airfares (guess this qualifies for the business discussion) and I realized I don't know which ai...
- Wed May 07, 2003 8:38 am
- Forum: Techniques and Tools
- Topic: Photos of Sandblasted and Firepolished Glass
- Replies: 19
- Views: 18349
Interesting pictures Steve and good investigating too. Thanks to Nikki and Tony too. Looks like the silicon carbide grit is blasting deeper holes in the glass that seal over with firepolishing trapping air. Ron Hi Ron and Steve, Nikki also showed me those photos - but in my experience, fire-polishi...
- Wed May 07, 2003 8:02 am
- Forum: Business Topics
- Topic: Copyright violation - illegal and unethical
- Replies: 31
- Views: 37671
](*,) As you know from our prior conversations, this has been a serious issue in my book for well over a year now. Sorry that you personally have now felt another part of this whole issue. As many of you know, I do alot of art/craft shows every year and I am appalled at the lack of ethics within th...
- Tue May 06, 2003 8:32 am
- Forum: Business Topics
- Topic: Copyright violation - illegal and unethical
- Replies: 31
- Views: 37671
Copyright violation - illegal and unethical
After much thought, I believe that this information needs to be aired in this forum. I post it as a reminder for those tempted, and as an educationnal posting for those who might somehow not know, that it is legally and ethically wrong to use pictures of work designed and created by others, without ...
- Wed Mar 19, 2003 8:44 am
- Forum: Techniques and Tools
- Topic: stands for display
- Replies: 12
- Views: 16636