Search found 8 matches
- Sat Nov 28, 2015 6:05 pm
- Forum: Techniques and Tools
- Topic: SUDDENLY ...air bubbles..SUGGESTIONS PLEASE?
- Replies: 3
- Views: 5548
SUDDENLY ...air bubbles..SUGGESTIONS PLEASE?
I've been full fusing 7 inch plates for years, using the same schedule. I use a small hot start kiln that doesn't allow much in terms of controlling the heat, ramp speed, etc. I use a tiny amount of glue to hold the top and bottom pieces in place. Suddenly there are "bubbles" under the top...
- Sat Sep 26, 2015 8:22 pm
- Forum: Techniques and Tools
- Topic: decal firing schedule suggestions? THANK YOU for any help
- Replies: 2
- Views: 3927
Re: decal firing schedule suggestions? THANK YOU for any help
I appreciate your response. I keep seeing work without that "stuff" so I still feel like I might be missing something. The results are disappointing and I see such beautiful pieces by other.
THANKS!
THANKS!
- Sat Sep 26, 2015 3:27 pm
- Forum: Techniques and Tools
- Topic: decal firing schedule suggestions? THANK YOU for any help
- Replies: 2
- Views: 3927
decal firing schedule suggestions? THANK YOU for any help
Decal Question...ANY help greatly appreciated I am using black low fire decals on a small 2 layered glass piece and firing it in my small hot start kiln. The thermostat doesn't give me many options for controlling the firing schedule. I fired the first time using the decal instructions which indicat...
- Thu Sep 17, 2015 1:23 pm
- Forum: Techniques and Tools
- Topic: Gold mermaid decals!
- Replies: 1
- Views: 3220
Gold mermaid decals!
I'm wondering if anyone knows where I can order gold mermaid fusible decals? I'm hoping to make a gift for my nieces' baby shower. thanks for any suggestion.
- Thu Nov 20, 2014 5:49 pm
- Forum: Techniques and Tools
- Topic: painting on glass
- Replies: 6
- Views: 10612
painting on glass
i am making tiny fused glass angel ornaments and would like to paint delicate eyes on their faces. i'm wondering about what kind of paint would work? can i paint before i fire the piece? or are there some type of markers that would last that i could put on afterwards?
thanks!
thanks!
- Thu Jun 27, 2013 6:16 am
- Forum: Techniques and Tools
- Topic: found metal for inclusion
- Replies: 2
- Views: 3896
found metal for inclusion
I am making a fused glass mezzuah as a wedding gift. the glass is recycled from part of the wedding ceremony so i can't really experiment too much. on the day of the wedding i found a heart shaped piece of metal and would like to include it. I have NO idea what type of metal it is. i'm not sure if t...
- Tue Sep 11, 2012 8:50 pm
- Forum: Jewelry Making
- Topic: fusible yoga decals? (ohm maybe or namaste)
- Replies: 5
- Views: 10092
Re: fusible yoga decals? (ohm maybe or namaste)
i would love to make my own, but have never done that...how can i get info about making my own decals? no luck with paper hole punches or i would use slide..thanks for any suggestions
- Sat Aug 25, 2012 12:51 pm
- Forum: Jewelry Making
- Topic: fusible yoga decals? (ohm maybe or namaste)
- Replies: 5
- Views: 10092
fusible yoga decals? (ohm maybe or namaste)
does anyone know of a place that sells decals with a yoga "theme"? I've found every other type of decal but this.
thanks for any suggestions.
thanks for any suggestions.