Search found 64 matches
- Tue Nov 07, 2023 5:49 am
- Forum: Techniques and Tools
- Topic: belts
- Replies: 2
- Views: 15739
Re: belts
I had a whole box of 5 104 inch CRL belts, every one of them broke, I order from HIS glassworks now and no trouble.
- Tue Nov 07, 2023 5:22 am
- Forum: Techniques and Tools
- Topic: Denver Kilns?
- Replies: 3
- Views: 13650
Re: Denver Kilns?
I have one, it's been good for last 10 years, only thing I replaced was a thermocouple last year. I use it almost every day.
- Sat Jul 22, 2023 2:59 pm
- Forum: Techniques and Tools
- Topic: Fiber Kiln/Shelf
- Replies: 11
- Views: 38476
Re: Fiber Kiln/Shelf
I have a Denver fiber kiln and 3 brick kilns. Firing in the fiber kiln is similar, the lid is fiberboard, the sides are the usual fluffy fiber wool. Call Jen Ken, they will advise you. Sorry you had runaway kiln.
- Mon Aug 15, 2022 2:43 am
- Forum: Techniques and Tools
- Topic: how to use this glass cutting tool?
- Replies: 5
- Views: 10390
Re: how to use this glass cutting tool?
Thanks Kevin! I didn't know about guiding with your finger. Even from this old post. Guess I haven't been studying the Warm Glass board like I used to.
- Sun Aug 07, 2022 11:50 pm
- Forum: Techniques and Tools
- Topic: Denver Machinery thermocouple error
- Replies: 2
- Views: 4147
Re: Denver Machinery thermocouple error
That's the one! OK, I'll try them- The response from Red LIon was really fast, here it is: "The OPEN error can mean a open thermocouple sensor or a hardware failure of the control given it's age. Thermocouples types are based on lead wire color code. TYPE J for example is RED and White leads. T...
- Sun Aug 07, 2022 5:58 pm
- Forum: Techniques and Tools
- Topic: Sandblast grit
- Replies: 6
- Views: 8869
Re: Sandblast grit
I got some on Amazon, even mailed Prime to Hawaii. Automotive shops have sandblasters, too, and will blast a piece for you if you are just getting rid of a scummy back or something coarse like that
- Sun Aug 07, 2022 5:50 pm
- Forum: Techniques and Tools
- Topic: Denver Machinery thermocouple error
- Replies: 2
- Views: 4147
Denver Machinery thermocouple error
I have error message "OPEN" on my 17 year old KL50DD Denver kiln. The manual on the Red Lion controller says it is the probe, which I assume is the thermocouple. Since Denver Machinery is not in business, I wonder how to find out how to get another thermocouple and how to install it. It is...
- Sat Feb 22, 2020 8:03 pm
- Forum: Techniques and Tools
- Topic: Fiber Kiln/Shelf
- Replies: 11
- Views: 38476
Re: Fiber Kiln/Shelf
I never had any luck with a hardened fiber shelf. The first firing was fine, the next one stuck like crazy and tore a pit out of the shelf making it worse than useless because the glass was ruined as well. If you have a fiber shelf, I would always use thin fire. But I agree with Kevin, a regular she...
- Fri Oct 25, 2019 4:57 am
- Forum: Techniques and Tools
- Topic: zyp coating
- Replies: 13
- Views: 18248
Re: zyp coating
I tried brushable ZYP boron nitride on fiber molds. It releases one time, firing up to fuse temperature the next time results in the coating sticking to the glass as a hazy film. Zyp has to be removed and replenished with a fresh coat which is pretty impossible on fiber.
- Mon Dec 17, 2018 8:24 pm
- Forum: Techniques and Tools
- Topic: Where is the iridescent 96?
- Replies: 7
- Views: 11124
Where is the iridescent 96?
Oceanside Glass doesn't appear to be manufacturing any iridized glass. Anyone have insight on that?
- Mon Oct 15, 2018 2:11 am
- Forum: Techniques and Tools
- Topic: Wetbelt sander belts breaking
- Replies: 10
- Views: 19857
Re: Wetbelt sander belts breaking
I had that happen with a batch of belts also, from CRL. They work for 15 minutes and then let go. They were a few years old when I got around to needing them. It was only one size that broke. I bought new different ones from HIS.
- Sat Jul 22, 2017 2:29 am
- Forum: Techniques and Tools
- Topic: Super Spray A Reaction, Shadows, Polishing
- Replies: 5
- Views: 9457
Re: Super Spray A Reaction, Shadows, Polishing
I have taken pieces to be sandblasted to an automotive machine shop. They use big blasters to clean parts and may be happy to sandblast your piece inexpensively. They don't do delicate decals, but an overall blast is not out of the question.
- Tue Jul 12, 2016 3:58 am
- Forum: Newcomer Forum
- Topic: New Tutorial using Clear Glass
- Replies: 1
- Views: 6151
Re: New Tutorial using Clear Glass
Thanks for posting! That's a lively piece of art.
- Fri May 20, 2016 6:46 pm
- Forum: Techniques and Tools
- Topic: Crazy Crusher
- Replies: 8
- Views: 14259
Re: Crazy Crusher
HI Terry, Do you have a picture of the cement mixer mill? I want to try this, I use a lot of frit about the size of a dime. Where did you get the stainless balls? What size are they?
- Fri May 20, 2016 3:36 am
- Forum: Techniques and Tools
- Topic: Devit Spray and Dichoric
- Replies: 4
- Views: 8548
Re: Devit Spray and Dichoric
Yes, it is likely. Better to make a test strip with materials you intend to use. Devit spray can be blotchy or change the color of the dichroic.
- Thu May 12, 2016 5:46 am
- Forum: Techniques and Tools
- Topic: SPECTRUM GLASS CLOSING DOWN
- Replies: 29
- Views: 92284
Re: SPECTRUM GLASS CLOSING DOWN
I am shocked, now what? That's a big loss for art glass world wide.
- Sun Mar 27, 2016 4:18 am
- Forum: Techniques and Tools
- Topic: Crazy Crusher
- Replies: 8
- Views: 14259
Re: Crazy Crusher
Can it make chips the size of a dime also? I'm currently crushing a 24x48 inch sheet with a pestle made of pipe in a stainless steel basin of water. I can do 1/8 sheet at a time. I made a finer frit crusher from directions here on the board with a jewelry press with an added an electric motor. It su...
- Fri Nov 20, 2015 4:11 am
- Forum: Techniques and Tools
- Topic: Bowl Slumping Questions
- Replies: 7
- Views: 15771
Re: Bowl Slumping Questions
that bowl shape is not particularly elegant finished as the bowl will slump far down into it and be mostly flat with a small upturned edge and possibly an uneven bottom. As it was mentioned, it isn't really made for fusing and presents a lot of problems with shifting off center, which is a real hear...
- Sun Feb 22, 2015 3:57 am
- Forum: Techniques and Tools
- Topic: Bee Wet Belt Sander refurbishing
- Replies: 9
- Views: 11571
Re: Bee Wet Belt Sander refurbishing
The duct tape works amazingly well. no wandering belts, runs pretty quiet, too. Thanks again Kevin, Marty , your admonishment well taken. I have been mostly religious to take off the tension, thanks for way earlier advice from you guys.
- Fri Feb 20, 2015 7:52 pm
- Forum: Techniques and Tools
- Topic: Bee Wet Belt Sander refurbishing
- Replies: 9
- Views: 11571
Re: Bee Wet Belt Sander refurbishing
I put on the duct tape already, works great! New belt, too, and I brushed off the upper assembly, I'll rinse it off real good after this session and take a look with the flashlight. The machine is not especially loud so I'm hoping the bearings are in good shape still. Funny about the belts, some are...