Tekta and Fiber Paper
I know some people, including me, have found a haze on Tekta after firing on Thinfire. I wondered if anyone had had any problems with fiber paper or is this an entirely different product? I want to fuse a plate with pattern bar slices in the center and a border of 6 mm Tekta. I'll fire directly on t...