Re: quality glass cutter
I think a lot has to do with your arm, wrist and shoulder strength (probably height is a factor as well). For me, an aging woman who has cut glass with almost every cutter ever made, I wouldn't take a million dollars for my MacInnes Glass Cutter, sold exclusively at Sunshine Glass works. They are sp...
- Mon Jan 26, 2015 8:09 pm
- Forum: Techniques and Tools
- Topic: Quenching glass
- Replies: 22
- Views: 26754
Re: Quenching glass
Once again, I would just like to say THANK YOU SO VERY MUCH! I have been all over the internet and You Tube (couldn't remember the word "quenching") and at last you have given me the tools here that I was seeking.
Bert you remain my eternal hero.
In gratitude!
Jolinda Marshall
Bert you remain my eternal hero.
In gratitude!
Jolinda Marshall
- Mon Mar 25, 2013 9:09 pm
- Forum: Techniques and Tools
- Topic: Tile saw question
- Replies: 27
- Views: 28499
Re: Tile saw question
Dana, In response to your question about the MK 370 EXP tile saw...be sure to order the one with the metal table. This is only offered on the EXP or I would order one as a replacement table for my 370. Both my husband and I have a 370 and BOTH have now warped so much in the middle of the table (sags...