Search found 5 matches
- Fri Apr 02, 2004 1:27 am
- Forum: Techniques and Tools
- Topic: Back Magic and slumping
- Replies: 7
- Views: 8938
Back Magic and Slumping
I appreciate the ideas. Guess I will have to rethink the situation. By the way, am I the oldest amaetur on the board? --76 --and still fusing and slumping.
- Thu Apr 01, 2004 9:12 pm
- Forum: Techniques and Tools
- Topic: Back Magic and slumping
- Replies: 7
- Views: 8938
Brock The texture is ok but there is a dullness about the piece that I thought to brighten. Actually they were already slumped but did now get to the desired shape. The temp then was 1225 and the time was 45 min. I understand that successive slumps require longer time and higher temp. Is this correc...
- Thu Apr 01, 2004 8:59 pm
- Forum: Techniques and Tools
- Topic: Back Magic and slumping
- Replies: 7
- Views: 8938
Back Magic and slumping
I have some plates that I want to brighten the botton of. I plan to use Back Magic and to cure it at 1000. Then I want to slump them at 1250 for 1&1/2 hours. Can i do this with the cured side against the mold with out a problem?
- Sat Apr 05, 2003 5:40 pm
- Forum: Techniques and Tools
- Topic: Kiln Wash Won't stick in mold
- Replies: 6
- Views: 8659
Kiln wash won't stick
As usual the board has come through. This is the first time I have experienced this in a little over 18 months of doing glass. Thanks to all.
Happy Ross
Happy Ross
- Sat Apr 05, 2003 3:56 pm
- Forum: Techniques and Tools
- Topic: Kiln Wash Won't stick in mold
- Replies: 6
- Views: 8659
Kiln Wash Won't stick in mold
I have a new ceramic mold and the BE kiln wash will not stick to one small spot. I even tried leaving a thin puddle over the spot when I baked it, but no good, it came right off. What should I do to make it stick?
Hopefully, Ross
Hopefully, Ross