Search found 65 matches
- Sat Apr 06, 2013 6:05 pm
- Forum: Techniques and Tools
- Topic: Bubble Repair?
- Replies: 8
- Views: 13047
Re: Bubble Repair?
I just fired 2 blanks, one 14" and the other 16". I ended up with many bubbles in the center of each, which had shards and stringer design. Clear cap on top of shard area and a bubble squeeze in the fireing. I drilled out the bubbles and filled them with fine clear frit. After a re-fire, t...
- Mon Apr 01, 2013 4:50 pm
- Forum: Techniques and Tools
- Topic: Bullseyeglass.com
- Replies: 3
- Views: 4690
Re: Bullseyeglass.com
Thanks Cynthia for the advise. I'll drive into town and try to find a signal somewhere. I have a love/hate relationship with living in the country. No cable or high speed phone and if I want to cook something a little bit exotic I have to cart the ingredients up here. But, it is beautiful on my moun...
- Mon Apr 01, 2013 3:48 pm
- Forum: Techniques and Tools
- Topic: Bullseyeglass.com
- Replies: 3
- Views: 4690
Bullseyeglass.com
I wasn't sure where to post this. I use a tablet when I'm at my studio, as I have no other internet hook-up. I need to go on the Bullseye site, and it keeps kicking me off. I seem to be able to get on line to other sites, but not their's. I've never had this problem before. Anyone else experiencing ...
- Sat Jul 21, 2012 5:39 pm
- Forum: Techniques and Tools
- Topic: Bead Door on Kiln
- Replies: 16
- Views: 19868
Re: Bead Door on Kiln
I didn't know they had a bead door option for a large kiln. Having such a large kiln so close to you while you are torching could be really hot. I use a Caldera for my bead making. It's 8" square, and is the perfect size for the amount of beads I can make in a 4, 6 or 8 hour session. The Calder...
- Sun Jul 15, 2012 3:10 pm
- Forum: Techniques and Tools
- Topic: Assistance with color options....
- Replies: 19
- Views: 22006
Re: Assistance with color options....
You won't get that vibrant purple/hot pink color with Sys 96. I use enamels when I make my flower tiles. Right now I am using Thompson's, as that is what I have on hand. Some of the other brands, Ferro or Reuche, may have a more extensive color selection.
Cate