firing problem
I have a Glassglow Model 300 kiln.It has worked beautifully for me for 8 years, so I bought another one, and I am having some issues with the new one. The builder of the kiln told me it may have something to do with the fact that different bricks were used for this new kiln (because the manufacturer...