follow-up: fusing flat a slumped piece and re slumping
Thanks to everyone for their input,I fused the slumped piece flat, I fused at 400 to 1050 held for 25min.,250 to1250 held 10min.,400 to 1400 held 5min. There is no variation in the thickness,and no apparent change in size,at least that I can see.However ,there are the slump marks on the back(bottom)...
- Wed Apr 30, 2003 1:44 pm
- Forum: Techniques and Tools
- Topic: What happens in a full fuse in a slumping mould?
- Replies: 19
- Views: 23456
Thanks to all
I appreciate the input.
I will refuse flat rather than in the mould,and go relatively slow
and expect (exactly) what everyone said!!!!
Mahalo.......
Mike
I will refuse flat rather than in the mould,and go relatively slow
and expect (exactly) what everyone said!!!!
Mahalo.......
Mike
- Tue Apr 29, 2003 4:08 pm
- Forum: Techniques and Tools
- Topic: What happens in a full fuse in a slumping mould?
- Replies: 19
- Views: 23456
What happens in a full fuse in a slumping mould?
I have been told that I probably shouldn't re-fuse a piece flat,that has been fused & slumped(variations in thickness issue).Can I fuse to about 1400 to fire polish in the orignal
mould without any thing weird happening,What should I expect?
Mahalo.....Mike
mould without any thing weird happening,What should I expect?
Mahalo.....Mike
- Tue Apr 29, 2003 1:54 pm
- Forum: Techniques and Tools
- Topic: Lost etched design while slumping.How to proceed?
- Replies: 14
- Views: 12288
- Mon Apr 28, 2003 12:52 pm
- Forum: Techniques and Tools
- Topic: Lost etched design while slumping.How to proceed?
- Replies: 14
- Views: 12288
- Sun Apr 27, 2003 3:38 pm
- Forum: Techniques and Tools
- Topic: Lost etched design while slumping.How to proceed?
- Replies: 14
- Views: 12288
- Sun Apr 27, 2003 1:59 pm
- Forum: Techniques and Tools
- Topic: Lost etched design while slumping.How to proceed?
- Replies: 14
- Views: 12288
Lost etched design while slumping.How to proceed?
I had two nicely fused pieces of Spectrum that I etched designs on(actually shaded) and slumped to 1250 and held 12 min.I lost all of the design( barely visible) Thats history,I learned a lesson.My question is now that they are slumped I cannot apply a resist to the slumped shape .Should I re-fuse t...