Search found 40 matches
- Wed Aug 14, 2013 8:07 pm
- Forum: Techniques and Tools
- Topic: Hanging a fused glass panel
- Replies: 4
- Views: 6927
Hanging a fused glass panel
I made a glass panel for a friend and she plans to hang it in a window-opening in between her dining room and kitchen. The glass is small enough that there is a 1 3/4" margin around the opening. My question is the method of hanging. I have been looking at clamps, two top and two bottom but ther...
- Sun Aug 04, 2013 7:44 pm
- Forum: Techniques and Tools
- Topic: Thinfire residue
- Replies: 6
- Views: 9603
Re: Thinfire residue
No, Bullseye clear. After a bit of research, I think I know what I did. I held it too long at the top full fuse temp. It's a big piece and I was worried it wouldn't fill in the gaps for the carving technique. I do have some areas in the big piece that has a film. Am looking into sandblasting service...
- Sun Aug 04, 2013 4:04 pm
- Forum: Techniques and Tools
- Topic: Thinfire residue
- Replies: 6
- Views: 9603
Re: Thinfire residue
I've used it for years and just bought the large roll of Bullseye thinfire! I really only had an issue one time with opal powder blue but this is Bullseye clear. This is frustrating to say the least. Does anyone have a way, other than sandblasting, to get it off? I have a large piece that I fired wi...
- Sun Aug 04, 2013 1:23 pm
- Forum: Techniques and Tools
- Topic: Thinfire residue
- Replies: 6
- Views: 9603
Thinfire residue
I'm having an issue with bullseye thin fire leaving a residue on the underside of my glass. The picture shows the whitish haze on the part that is against the thinfire. No haze where 1/16" fiber paper is used. Any suggestions? http://i1291.photobucket.com/albums/b551/Alice_Benvie_Gebhart/image_...
- Mon Jul 29, 2013 5:54 pm
- Forum: Business Topics
- Topic: Pricing for interior designers and design firms
- Replies: 6
- Views: 9962
Re: Pricing for interior designers and design firms
Thank you all. Very helpful.
- Mon Jul 08, 2013 3:33 pm
- Forum: Business Topics
- Topic: Pricing for interior designers and design firms
- Replies: 6
- Views: 9962
Re: Pricing for interior designers and design firms
Thanks guys. This gives me a great perspective. I would like to work with professionals in the field, if possible, but don't want to give it away either. I was given a 40% discount by well-known lighting craftspeople being that I was an artist and they were artists and was overjoyed by that. Didn't ...
- Mon Jul 08, 2013 4:55 am
- Forum: Business Topics
- Topic: Pricing for interior designers and design firms
- Replies: 6
- Views: 9962
Pricing for interior designers and design firms
Well, I have been contacted by some different design firms who have seen different pieces online asking for a "designers discount" if they purchase a piece for a client. Not sure how to approach this. Is a wholesale rate of 50% off retail common in these cases? What are your practices? I w...
- Sat Jun 22, 2013 10:54 am
- Forum: Techniques and Tools
- Topic: New Kiln Tests and Trials
- Replies: 4
- Views: 5817
Re: New Kiln Tests and Trials
Thanks Bert. I saw that on Warm tips and thought that as an option for the lid. I do have a cathedral-type ceiling and can find the beams easily.
- Fri Jun 21, 2013 8:37 pm
- Forum: Techniques and Tools
- Topic: New Kiln Tests and Trials
- Replies: 4
- Views: 5817
New Kiln Tests and Trials
I just bought a new GF8CS kiln. It took awhile to get it and get it up and running and have a few questions for the exports. Firstly, I am looking into getting a hoist to help with lifting the lid. I reviewed the warm tips for a pulley system and that was helpful. I also looked into using a pulley a...
- Fri Jun 07, 2013 8:08 pm
- Forum: Techniques and Tools
- Topic: tile saw issue
- Replies: 9
- Views: 11475
Re: tile saw issue
Thanks for options.
- Fri Jun 07, 2013 2:45 pm
- Forum: Techniques and Tools
- Topic: tile saw issue
- Replies: 9
- Views: 11475
Re: tile saw issue
Using Husqvarna SuperLock Glass Plus diamond blade.
The saw goes along fine, cut is great then all of a sudden it seems to jump and blade seems to skid across top and spark.
The saw goes along fine, cut is great then all of a sudden it seems to jump and blade seems to skid across top and spark.
- Fri Jun 07, 2013 1:06 pm
- Forum: Techniques and Tools
- Topic: tile saw issue
- Replies: 9
- Views: 11475
tile saw issue
I have a DeWalt D24000 which has a 10" blade but the problem I am having I had with a saw I had at the beginning of my glass career. I'd just like to know what is going on. I am cutting and it is just fine but then it seems to pull the glass quickly through the cut and not cut all the way throu...
- Tue Feb 19, 2013 1:22 pm
- Forum: Techniques and Tools
- Topic: New Kiln suggestions
- Replies: 0
- Views: 17148
New Kiln suggestions
Hi friends, I wish to purchase a new and larger kiln. I have been looking at the Denver kiln KL-50 which is 30 x 60 x 12 interior and the Olympic GF-10 which is 30 x 48 x 12 interior. Both are about the same price. I am looking for a new kiln so I can work larger and use it for classes but my primar...
- Thu Dec 20, 2012 1:26 am
- Forum: Photos and Stuff
- Topic: Quiet Sunset
- Replies: 14
- Views: 14765
Re: Quiet Sunset
Don't know why it got taken off.
Try this again.
Try this again.
- Tue Nov 27, 2012 10:08 pm
- Forum: Photos and Stuff
- Topic: Quiet Sunset
- Replies: 14
- Views: 14765
Quiet Sunset
I haven't posted in awhile as webshots has changed and my photos just wouldn't upload. I moved to photobucket and think this will work. My newest piece is called Quiet Sunset and I did it as a commission. My client wanted trees, bright colors with purples, oranges and reds. I am pleased with the res...
- Thu Nov 01, 2012 10:28 pm
- Forum: Business Topics
- Topic: wholesalecrafts.com
- Replies: 5
- Views: 9019
Re: wholesalecrafts.com
Thanks Cheryl.
- Mon Oct 29, 2012 8:40 pm
- Forum: Business Topics
- Topic: wholesalecrafts.com
- Replies: 5
- Views: 9019
Re: wholesalecrafts.com
Just wondered what kind of things you sell and if it was lucrative for you.
- Sat Sep 22, 2012 10:12 pm
- Forum: Business Topics
- Topic: wholesalecrafts.com
- Replies: 5
- Views: 9019
wholesalecrafts.com
I have started to make some functional pieces as well as some items I may like to wholesale. I have been considering wholesalecrafts.com and was wondering if anyone has used them and has any advise for me.
- Fri Jul 06, 2012 10:56 pm
- Forum: Techniques and Tools
- Topic: Which glue is best for glass to glass on sushi plates?
- Replies: 17
- Views: 19547
Re: Which glue is best for glass to glass on sushi plates?
Throw the old silicone away. The silicone works great s long as it is not old. The only times it didn't work for me was because it hadn't set and that was because it was beyond its expiration date. So be careful of the old stuff.
- Fri Jul 06, 2012 5:49 pm
- Forum: Photos and Stuff
- Topic: Brave Reasons
- Replies: 17
- Views: 18395
Re: Brave Reasons
I have your amber one on my pinterest because I love it!
Alice
Alice