Search found 51 matches

by Melissa Terman
Fri Apr 05, 2019 5:39 pm
Forum: Techniques and Tools
Topic: Float Glass Reco Needed for Decals
Replies: 7
Views: 9127

Re: Float Glass Reco Needed for Decals

smoothness was the issue for the decals and the frit combined with keeping glass 3mm thick. You have to tack fuse frit quickly and at a lower temperature because it's so small and thin. We don't get to the higher temperature needed to get it smooth. I thought I had read that you could add small surf...
by Melissa Terman
Fri Apr 05, 2019 1:50 pm
Forum: Techniques and Tools
Topic: Float Glass Reco Needed for Decals
Replies: 7
Views: 9127

Re: Float Glass Reco Needed for Decals

That's great information, thank you! Another question. Can you use bullseye frit on float glass? she wants to make an appearance of snow on the window. We did it with single layer 3mm bullseye without distortion to 1420F. Does the float act differently at that temperature? Is there some basic printe...
by Melissa Terman
Fri Apr 05, 2019 12:49 pm
Forum: Techniques and Tools
Topic: Float Glass Reco Needed for Decals
Replies: 7
Views: 9127

Float Glass Reco Needed for Decals

Hi, Note: I only have experience using Bullseye Glass for fusing. I have a student/friend who wants to make small windows for her dollhouse using fusible decals for a pattern. She needs the glass to remain thin (3mm) and smooth. Can't bring Tekta to a full fuse to get it smooth for decal placement a...
by Melissa Terman
Fri Apr 16, 2004 8:48 am
Forum: Business Topics
Topic: Urban Glass-Glassblower's Ball & Auction
Replies: 6
Views: 10665

I'll look for you there. But if you figure out who I am first, please say hi.
by Melissa Terman
Sun Mar 21, 2004 7:01 pm
Forum: Business Topics
Topic: Bullseye catalog
Replies: 20
Views: 42310

I didn't get mine either, although they asked me three times to confirm my address.
by Melissa Terman
Sat Mar 20, 2004 6:34 pm
Forum: Techniques and Tools
Topic: Respirator ?
Replies: 4
Views: 5941

Cynthia, Purple filters? Mine are pink. I thought we are supposed to use P100s. Please let me know if that is wrong. Camaro, I use a vaccum (sp?) with a HEPA filter, especially for fiber papers. Otherwise, all the dust is pushed back out into the air. I purchased a Shark brand from Bed, Bath & B...
by Melissa Terman
Sat Mar 20, 2004 2:26 pm
Forum: Techniques and Tools
Topic: Drilling finished dichroic pieces?
Replies: 18
Views: 21028

Melissa that is brilliant! Did you come up with it yourself!!!!?? Thank you Amy. I would love to take credit for being brilliant, instead I will have to say that I am an astute student. I've taken all I've learned here on this fantastic board, plus all I've learned from my metals teachers mixed wit...
by Melissa Terman
Sat Mar 20, 2004 1:19 am
Forum: Business Topics
Topic: Urban Glass-Glassblower's Ball & Auction
Replies: 6
Views: 10665

Urban Glass-Glassblower's Ball & Auction

Will any of you be attending the Glassblower's Ball & Auction in New York on April 17th?

I have donated my "Oh Georgia!" jewelry piece and will be in attendance.

Image

Please let me know. I would love to say hi.

Melissa
by Melissa Terman
Sat Mar 20, 2004 1:13 am
Forum: Business Topics
Topic: See-Through Concrete
Replies: 4
Views: 7865

Geri,

Thanks for posting that info. It's fantastic!!!

Melissa
by Melissa Terman
Sat Mar 20, 2004 1:05 am
Forum: Techniques and Tools
Topic: Drilling finished dichroic pieces?
Replies: 18
Views: 21028

I know you probably have all the info you need to create holes, but I thought I might add my 5cents (inflation and all). I use a spring gauge (a caliper type tool) to mark piece both front and back using a sharpie. Then I wax the sharpie mark (candle or chapstick works) so it won't come off in water...
by Melissa Terman
Fri Mar 12, 2004 7:20 pm
Forum: Photos and Stuff
Topic: New Sink just delivered
Replies: 20
Views: 27954

It's awesome. I am soooooo jealous of you for making a sink that is so beautiful and I am jealous of the people who get to see and use it everyday.

Melissa (she who wishes she could make sinks)
by Melissa Terman
Thu Mar 04, 2004 5:23 pm
Forum: Techniques and Tools
Topic: Perfect white for fusing( Liquid Paper???) YES
Replies: 40
Views: 47142

Fun Fact: Michael Nesmith's (of Monkees fame) mother invented Liquid Paper (aka White Out). When she invented this stuff to benefit the typing community, she had no idea what it would do for the arts as well. FYI-In the "At The Bench" section of AJM magazine (Feb 2004), Alan Revere recomme...
by Melissa Terman
Thu Feb 12, 2004 11:57 pm
Forum: Techniques and Tools
Topic: Jen-Ken Kiln question
Replies: 12
Views: 13047

Alas, I am windowless. But I am glad I didn't fork over the extra dough because I had to have an electrician come in and futz with my wiring and install a 120/20 outlet even though it runs on household current. That was expensive! And being a glassblower too, I find it oddly refreshing to get the bl...
by Melissa Terman
Sat Feb 07, 2004 9:30 am
Forum: Business Topics
Topic: Current Price of Silver and gold
Replies: 10
Views: 15121

Hi Geri, Go to the very bottom of your "MY Yahoo" page. On the right sight, you will see "add right side content" pull down menu. It's called "currency converter". Add the currency you wish to track. Gold, silver, palladium, etc. are listed in the currencies. Darn! Silv...
by Melissa Terman
Fri Feb 06, 2004 1:02 am
Forum: Business Topics
Topic: Current Price of Silver and gold
Replies: 10
Views: 15121

I have a customized Web Page with Yahoo called My Yahoo. When I launch Internet Explorer, this page comes up. I have all the info I want pushed to me (i.e., my stocks, my horoscope, my incurable need for entertainment gossip). On this page I also have a currency converter so I can check how the %^&a...
by Melissa Terman
Fri Feb 06, 2004 12:44 am
Forum: Photos and Stuff
Topic: A little splash of color
Replies: 30
Views: 33079

Sleek!

Beautiful finish.

Mel
by Melissa Terman
Sun Jan 18, 2004 6:53 pm
Forum: Techniques and Tools
Topic: The dreaded revisiting of artists statements . . .
Replies: 9
Views: 9103

I admire you for being so gutsy as to put yourself on the line and ask for help, thus criticism. I doubt I could do it. So kudos to you. In my former life, I was a professional copywriter and then an executive at an advertising agency. I just want to relate to you what goes through my head when read...
by Melissa Terman
Thu Jan 15, 2004 1:36 pm
Forum: Techniques and Tools
Topic: Nichrome Wire Turned Black
Replies: 8
Views: 10274

No matter how weird it gets, it never gets weird enough for me... Please, no advice that includes odd rituals, praying, incantations and/or sacrifices. Sheesh, make up your mind, lady! Jerry, I thought I did make up my mind. I don't like appeasing unknown forces, but I do enjoy the bizarre. Merely ...
by Melissa Terman
Wed Jan 14, 2004 5:34 pm
Forum: Techniques and Tools
Topic: Nichrome Wire Turned Black
Replies: 8
Views: 10274

Nichrome Wire Turned Black

Recently, I read on the board a recommendation for nichrome wire. It's supposed to stay shiny? Mine turned black. I actually like the result, but it was not what I was planning on. If I want it shiny, what does a girl have to do? Please, no advice that includes odd rituals, praying, incantations and...
by Melissa Terman
Fri Jan 02, 2004 10:13 pm
Forum: Techniques and Tools
Topic: Hey, where'd it go?
Replies: 1
Views: 3169

Hey, where'd it go?

This never happended before: After using a preferred preprogrammed firing schedule, when I opened my Jen-Ken Maxi Fuser (13" round shelf), I found 2 small jewelry pieces, fully formed, at the bottom of the kiln (under the kiln shelf). Stats: 2 layers of BE @ 3mm with fine silver surface inclusi...