by Michael McNerney
Tue Apr 13, 2004 11:26 am
Forum: Photos and Stuff
Topic: Fused Panels for my back splash
Replies: 7
Views: 12364

Phil,
Good Guess.
They are Black Bullseye with mica applications and Dichro Beads.

Michael
by Michael McNerney
Tue Apr 13, 2004 7:59 am
Forum: Techniques and Tools
Topic: fusing with lava cloth problems help please!!!!!!!!!!!!
Replies: 17
Views: 21093

Rhonda,
Check out my pics on the picture page. "Fused Panels"
I fired these on thin Fire and have little or no texture at all on the backs and had no problem hanging them.

Michael
by Michael McNerney
Tue Apr 13, 2004 7:48 am
Forum: Photos and Stuff
Topic: Fused Panels for my back splash
Replies: 7
Views: 12364

Being hung

by Michael McNerney
Tue Apr 13, 2004 7:47 am
Forum: Photos and Stuff
Topic: Fused Panels for my back splash
Replies: 7
Views: 12364

Fused Panels for my back splash

Hello everyone.
I just wanted to share my current project with you all and get your feed back.

http://groups.msn.com/McNerneyGlassAlbu ... PhotoID=13

Thanks
Michael
by Michael McNerney
Wed Apr 07, 2004 2:27 pm
Forum: Techniques and Tools
Topic: This link may be helpful
Replies: 1
Views: 3698

This link may be helpful

by Michael McNerney
Wed Mar 17, 2004 3:03 pm
Forum: Techniques and Tools
Topic: Warm Glass Weekend Update
Replies: 49
Views: 62502

Hey Ron Coleman
I found a flight from columbus to elmira for about $182 roundtrip on US Airways. Do ya wana share a rent a car from elmira to corning?

Michael
by Michael McNerney
Tue Mar 16, 2004 10:26 am
Forum: Techniques and Tools
Topic: Mica and Kylr-Fire (anyone tried it)
Replies: 24
Views: 24460

Robyn,
I have had no success trying to screen micas and klyr fire. The mixture is to thin and spreads badly even using a high mesh screen. You need to find a mixing medium with a much thicker consistency that isnt toxic when you fire it.

Michael
by Michael McNerney
Tue Feb 24, 2004 12:55 pm
Forum: Techniques and Tools
Topic: Pot Melt ?
Replies: 2
Views: 3971

Pot Melt ?

Has anyone tried doing a pot melt onto fiber paper or Thin Fire?

Thanks
Michael
by Michael McNerney
Fri Feb 06, 2004 8:37 am
Forum: Techniques and Tools
Topic: Melting stringers?
Replies: 15
Views: 18215

daffodildeb, I also usually use a tea ight candle, Yes I do get soot. the soot will burn off during your fire. I do this with dichroic stringers all of the time and haven't had a problem yet. you can also go to the hardware store and buy a small plumbing torch if you dont want to invest into a lamp ...
by Michael McNerney
Thu Feb 05, 2004 4:24 pm
Forum: Photos and Stuff
Topic: A little splash of color
Replies: 30
Views: 33154

Hey Ron,
Is this the piece that you and I were discussing on the phone tuesday evening? It is wonderful, GREAT WORK

Michael
by Michael McNerney
Tue Dec 30, 2003 12:11 pm
Forum: Photos and Stuff
Topic: New Green Mica Bowl with Dichro Beads
Replies: 10
Views: 12785

Tony,
I was under the impression that there would be a chance of ingesting
the micas. I didnt want to poison my client base, but if there is little or no risk of ingestion put some pasta in them and have a party.


Thanks for the info Toney
by Michael McNerney
Tue Dec 30, 2003 12:05 pm
Forum: Photos and Stuff
Topic: New Green Mica Bowl with Dichro Beads
Replies: 10
Views: 12785

UPDATE:

Thank you all for your interest and insight

UPDATE:This piece sold two weeks ago.

Michael
by Michael McNerney
Tue Dec 30, 2003 12:02 pm
Forum: Photos and Stuff
Topic: New Green Mica Bowl with Dichro Beads
Replies: 10
Views: 12785

Nita, I fused the clear and black together first, then applied mica's. Capping micas can be kind of tricky, if ther kiln is to hot they sink and disapear, to cool and they can create air bubbles in you cap. So I say why risk it, put them on top and tell your buyer not to eat off of it. Some things a...
by Michael McNerney
Tue Dec 23, 2003 2:32 pm
Forum: Techniques and Tools
Topic: Just in the festive holiday spirit
Replies: 3
Views: 4603

Just in the festive holiday spirit

Fuse they told me pa rum pum pum pum A new sheet of glass to cut, pa rum pum pum pum The tests and experiments are done. pa rum pum pum pum It's time to fire the kiln pa rum pum pum pum rum pum pum pum rum pum pum pum We are going up to ramp 1 pa rum pum pum pum, We'll crash the kiln before were don...
by Michael McNerney
Mon Dec 22, 2003 5:25 pm
Forum: Photos and Stuff
Topic: New Green Mica Bowl with Dichro Beads
Replies: 10
Views: 12785

I get them at prizm art supplies in columbus ohio.
They are better known as Pearl-EX Pigments
by Michael McNerney
Mon Dec 22, 2003 9:44 am
Forum: Photos and Stuff
Topic: New Green Mica Bowl with Dichro Beads
Replies: 10
Views: 12785

New Green Mica Bowl with Dichro Beads

New Green Mica Bowl with Dichro Beads

http://groups.msn.com/McNerneyGlassAblb ... &PhotoID=6

Any and all comments welcome

Thanks
Michael
by Michael McNerney
Thu Dec 18, 2003 2:27 pm
Forum: Techniques and Tools
Topic: Mica Paint Pixture
Replies: 7
Views: 8454

Tyler,
I hand draw my designs right on to the shelf paper then cutwith an exacto knife.
does that answer your question?

Michael
by Michael McNerney
Wed Dec 17, 2003 9:38 am
Forum: Techniques and Tools
Topic: Mica Paint Pixture
Replies: 7
Views: 8454

Tyler, No, Isopropyl alchohol to mix my powders Yes, I use from 8 to 15 coats Bullseye (just my favorite) Soap and Water Shelf paper or Cheep Contact Paper (very easy to transfer design or picture on to) You can see my applications! http://groups.msn.com/McNerneyGlassAblbum/shoebox.msnw Good Luck an...
by Michael McNerney
Thu Oct 30, 2003 10:45 am
Forum: Photos and Stuff
Topic: walpole stain on float
Replies: 9
Views: 10878

Where can I get some of this stain that I am reading about?
by Michael McNerney
Thu Oct 30, 2003 10:30 am
Forum: Photos and Stuff
Topic: I got the Micas down so lets try a post
Replies: 18
Views: 21771

Yes Jim,
They are all micas.
Silver, Purple and blue all applied at one time and fired.
Thanks for the feedback