Search found 17 matches
- Thu Jan 08, 2004 9:30 pm
- Forum: Kiln Casting
- Topic: Turning my potters wheel into a wet sander? Help!
- Replies: 14
- Views: 21802
Check out SW Diamond: http://swdiamond.freeyellow.com/ I bought one of their diamond discs a few years ago, and run it on an old electric potters wheel. The set up works great. The discs come with a magnetic backing so you need to attach a heavy piece of steel to the top of the potters wheel, which ...
- Fri Jan 02, 2004 12:53 pm
- Forum: Techniques and Tools
- Topic: Building a propane based infrared heat kiln
- Replies: 17
- Views: 19001
- Fri Jan 02, 2004 12:07 am
- Forum: Techniques and Tools
- Topic: Building a propane based infrared heat kiln
- Replies: 17
- Views: 19001
You ignore proper annealing at your own risk. Normally you should hold the piece at the annealing temperature for at least 15 minutes, and more if the piece has any thickness. Then cool to the strain point slowly, before a more rapid cool to room temperature. The exact schedule would be based on sev...
- Wed Dec 31, 2003 1:54 pm
- Forum: Techniques and Tools
- Topic: Building a propane based infrared heat kiln
- Replies: 17
- Views: 19001
- Wed Dec 31, 2003 12:35 am
- Forum: Techniques and Tools
- Topic: Building a propane based infrared heat kiln
- Replies: 17
- Views: 19001
Most glass would crack if heated that quickly. You might get away with heating small pierces of thin material, but I dont see how it could work on larger or thicker panels. Dont forget that if you paint on glass, the painted areas will absorb heat at a different rate than the clear, and each color w...
- Fri Jul 11, 2003 11:19 pm
- Forum: Business Topics
- Topic: Selling Art Glass From a Website
- Replies: 5
- Views: 7619
Selling Art Glass From a Website
Does anybody try to sell glass directly from their website? Or is the website just used for promation, and as a reference for shops and galleries that order wholesale? And if you do try to sell directly off the website, do you use a "shopping cart", which seems somewhat awkard for an indiv...
- Mon Jul 07, 2003 2:09 pm
- Forum: Kiln Casting
- Topic: Why Plaster Molds Crack
- Replies: 11
- Views: 20533
Why Plaster Molds Crack
I want to comment on the issue of why plaster/silica molds crack. It seems to me that a mold can only crack from internal stresses. In plaster/silica molds these stresses can only come from heating, and could generally come only from these causes: (1) Escaping moisture from a damp mold, or from the ...
- Sat Jun 28, 2003 9:18 pm
- Forum: Kiln Casting
- Topic: properties of mold materials
- Replies: 25
- Views: 33022
- Fri Jun 27, 2003 7:37 pm
- Forum: Kiln Casting
- Topic: Advice On A Mold For Casting A Head Sized Object
- Replies: 20
- Views: 27470
- Fri Jun 27, 2003 3:08 pm
- Forum: Kiln Casting
- Topic: Advice On A Mold For Casting A Head Sized Object
- Replies: 20
- Views: 27470
Marc: Thanks very much for all your help. I now know basically what I am going to try on my first attempt. One question. If I add 20% refractory cement, what should I expect in terms of the surface finish of the glass? I have a sandblaster, and could easily clean the casting up that way, but would p...
- Thu Jun 26, 2003 11:45 pm
- Forum: Kiln Casting
- Topic: Advice On A Mold For Casting A Head Sized Object
- Replies: 20
- Views: 27470
The annealing temperature is about 935 F, perhaps slightly higher for a casting. Fenton is basically just soda lime glass with a few added fluxes, but no lead. The kiln controller is separate. I realize that adding a castable cement would make the mold a lot tougher, but what happens after the casti...
- Thu Jun 26, 2003 9:26 pm
- Forum: Kiln Casting
- Topic: Advice On A Mold For Casting A Head Sized Object
- Replies: 20
- Views: 27470
I am planning to use a 50-50 mix of pottery plaster and silica for the mold, perhaps with some added fiberglass or ceramic fibre. It will be fired in a ceramic kiln with a ramp type controller. I was planning to use Fenton FHC cullet, but this could change. If I added cement to the plaster, what wou...
- Thu Jun 26, 2003 8:36 pm
- Forum: Kiln Casting
- Topic: Advice On A Mold For Casting A Head Sized Object
- Replies: 20
- Views: 27470
- Thu Jun 26, 2003 1:38 pm
- Forum: Kiln Casting
- Topic: Advice On A Mold For Casting A Head Sized Object
- Replies: 20
- Views: 27470
Thanks for the advice. Yes some heads are larger than others. But the head I am casting is actually a full size human skull. Death is said to be the great leveller......... Anyway, I have got to the point of making waxes from a rubber mold that in turn was made from a model. We took some liberties w...
- Thu Jun 26, 2003 11:05 am
- Forum: Kiln Casting
- Topic: Advice On A Mold For Casting A Head Sized Object
- Replies: 20
- Views: 27470
Advice On A Mold For Casting A Head Sized Object
I am planning to kiln cast a solid object about the size of a human head. I would like advice on the thickness of the walls of the mold. I want something thick enough to hold the weight of the glass without cracking, but at the same time I want to keep the overall dimensions down, to have a reasonab...
- Sun Mar 23, 2003 11:17 pm
- Forum: Techniques and Tools
- Topic: Slumping Into A Wok
- Replies: 5
- Views: 9321
- Fri Mar 21, 2003 3:35 pm
- Forum: Techniques and Tools
- Topic: Slumping Into A Wok
- Replies: 5
- Views: 9321
Slumping Into A Wok
I would appreciate feedback from anyone slumping into a wok. The wok I have is not stainless. Do you have problems with warpage, or scaling? What type of separator do you use? Does the wok deteriorate with multiple firings? Are there any other problems? Does anyone have experience with the boron nit...