I've been having a problem suddenly with my fiber paper. I bought a huge roll of it, and have had no problem at all, then suddenly it scorches in the kiln beginning at about 850F and affects the glass, as well. This is about halfway thru the roll. At first, I just cut the appropriate size, and put m...