Search found 2 matches

by Monika
Wed Apr 30, 2014 3:34 pm
Forum: Techniques and Tools
Topic: Bending 2mm Stringer
Replies: 12
Views: 14258

Re: Bending 2mm Stringer

Use a tea light, less heat, better control
by Monika
Fri Dec 14, 2007 1:53 am
Forum: Techniques and Tools
Topic: Crack in finished bowl
Replies: 3
Views: 13649

Re: Crack in finished bowl

Sue,
check your pm,