- Views: 13686
Slumping LARGE pc
Well it WAS only 9" deep, but since I'm working on this project I've ordered an extension for it, which will give me another 9". This project just turned into an add on after I had already made 2 pieces for other spots. The darn decorator talked him into the shape and size....and of couse ...
- Tue Mar 25, 2003 4:49 pm
- Forum: Techniques and Tools
- Topic: slumping large pc
- Replies: 10
- Views: 13686
Slumping Large
The pc will be in a kiln using top elements approx 3 1/2 away from top elements ( I hope this will work) I also have side elements in this kiln, but can only use either side or top due to power constrictions...hmm now that I think about it I have to use top elements since I am using the full width o...
- Tue Mar 25, 2003 11:36 am
- Forum: Techniques and Tools
- Topic: slumping large pc
- Replies: 10
- Views: 13686
- Mon Mar 24, 2003 11:25 pm
- Forum: Techniques and Tools
- Topic: slumping large pc
- Replies: 10
- Views: 13686
slumping large pc
I'm getting ready to slump over a mold ( drape), it's quite a bit larger than anything I've done so far. It has about a 25" diameter(2 full layers of BE with some areas 3 and 4 layers of BE thin), I'm trying to decide if I should go really slow from 1000 up to slump......or AFAP from 1000 on up...
- Sun Mar 23, 2003 1:13 am
- Forum: Techniques and Tools
- Topic: kiln builder?
- Replies: 0
- Views: 22118
kiln builder?
thinking (planning for the day I have $),any kiln builders close to San Clemente,CA. I'd love a Large kiln, maybe 65-70" x 22? 24