Search found 37 matches
- Fri Jan 17, 2014 2:40 am
- Forum: Photos and Stuff
- Topic: my 2 young birds
- Replies: 4
- Views: 7244
Re: my 2 young birds
Thank you Les for your comments. The feedback is so important! i was afraid that the birds were so frightening that no one dare to say a word..oy vey:) I created hinted birds sitting to rest on a kind of rock. next time i will try to make them more define as you suggested.In real life the birds look...
- Tue Jan 14, 2014 9:43 am
- Forum: Photos and Stuff
- Topic: my 2 young birds
- Replies: 4
- Views: 7244
my 2 young birds
A new work i made using pate de verre technique.
The big bird supposed to be me:)
(the work is hollow)
i would like to hear your remarks.
thank you
oritt
The big bird supposed to be me:)
(the work is hollow)
i would like to hear your remarks.
thank you
oritt
- Fri Jul 12, 2013 9:35 am
- Forum: Kiln Casting
- Topic: White - gray - pate de verre
- Replies: 12
- Views: 15106
Re: White - gray - pate de verre
Osnat,
Maybe the use of Less cmc can help.
cmc sometimes is the reason for a look of kind grey/not clean colour.
Maybe the use of Less cmc can help.
cmc sometimes is the reason for a look of kind grey/not clean colour.
- Thu May 30, 2013 7:47 am
- Forum: Photos and Stuff
- Topic: Chili hot pepper
- Replies: 11
- Views: 12391
Re: Chili hot pepper
I don’t know if there is another glass artist that succeeded to create chili hot pepper by using pate de verre technique. Maybe chili hot pepper were created by flame working but doing it with pate de verre is really unique. I was there and saw your struggle and the troubles you faced making it, and...
- Sun Apr 14, 2013 7:58 pm
- Forum: Photos and Stuff
- Topic: pate de verre
- Replies: 9
- Views: 12301
Re: pate de verre
God bless you cynthia!
you enriched my knowledge!
Thank you very very much!!!
you enriched my knowledge!
Thank you very very much!!!
- Sun Apr 14, 2013 9:48 am
- Forum: Photos and Stuff
- Topic: pate de verre
- Replies: 9
- Views: 12301
Re: pate de verre
Thank you Valerie . I love the fragile look of thin pate de verre(about 2mm). With the holes it seems like it is fragile but it is really strong inspite of the holes . I love the "wild" natural look of the piece like in this piece: http://glassquarterly.files.wordpress.com/2009/07/saare_wi...
- Sat Apr 13, 2013 10:11 pm
- Forum: Photos and Stuff
- Topic: pate de verre
- Replies: 9
- Views: 12301
Re: pate de verre
there are 2 things I would like to learn about pate de verre: 1.in the picture of the 2 faces there are holes between the frits. Is it ok? Or is it a fault? Looking to the piece through the light is nice to see the holes but is it ok? 2. in the blue picture I put more percent of powder so there is a...
- Sat Apr 13, 2013 1:12 am
- Forum: Photos and Stuff
- Topic: pate de verre
- Replies: 9
- Views: 12301
pate de verre
Hello friends,
i began using pate de verre technique.
here are my 3 first tries.
i would love to hear your comments and opinion inorder to find ways to improve my work,
thank you
oritt
i began using pate de verre technique.
here are my 3 first tries.
i would love to hear your comments and opinion inorder to find ways to improve my work,
thank you
oritt
- Tue Feb 19, 2013 1:30 am
- Forum: Photos and Stuff
- Topic: new work
- Replies: 15
- Views: 16137
Re: new work
Beautiful!!Beautiful!!Beautiful!!Beautiful!!
- Mon Feb 04, 2013 3:56 am
- Forum: Newcomer Forum
- Topic: Blew a fuse?
- Replies: 3
- Views: 5590
Re: Blew a fuse?
Hi Haley
sorry to hear about your kiln..
my colleague here had similar problem with her kiln.
she also made experiments reaching 1700 f .
the kiln manufacturer told her that she pushed the limits of the kiln and because of it it made the relay more vulnerable.
sorry to hear about your kiln..
my colleague here had similar problem with her kiln.
she also made experiments reaching 1700 f .
the kiln manufacturer told her that she pushed the limits of the kiln and because of it it made the relay more vulnerable.
- Sun Feb 03, 2013 5:55 am
- Forum: Newcomer Forum
- Topic: More about melts
- Replies: 9
- Views: 9966
Re: More about melts
Have you seen this site? It has several pot melts with before and after photos so you can get some idea of what they put in the pot. http://www.glassblower.info/pot-melt-pot-drop/warm-glass-hot-glass-unique-glass.html I've only done a few melts thus far. I've mixed transparents and opaques with goo...
- Tue Nov 13, 2012 8:33 am
- Forum: Techniques and Tools
- Topic: It cracked AGAIN!
- Replies: 24
- Views: 22239
Re: It cracked AGAIN!
maybe the high temp (1700) was the reason for the break in this earlier work too ?and not because it was stuck to the firebrick ?? http://www.warmglass.com/phpBB/viewtopic.php?f=2&t=39575 i agree with you less!! wonderful results can be achieved by reaching only 1500 temp. High temp can effect t...
- Tue Oct 02, 2012 12:45 am
- Forum: Photos and Stuff
- Topic: Uroboros Residency
- Replies: 44
- Views: 42268
Re: Uroboros Residency
Hi Les,
i am working and testing pate de verre using a kind of new mold.
When i get results i will send a picture:)
Take care
oritt
i am working and testing pate de verre using a kind of new mold.
When i get results i will send a picture:)
Take care
oritt
- Mon Oct 01, 2012 7:18 am
- Forum: Photos and Stuff
- Topic: Uroboros Residency
- Replies: 44
- Views: 42268
Re: Uroboros Residency
twin vision glass wrote:http://www.canadahouse.com/dynamic/artw ... rkID=29627 Yeah! it has found a home. Les
Congratulations les!!
it surely gives a lot of energy to make more beautiful creations:)
- Wed Aug 22, 2012 12:16 am
- Forum: Photos and Stuff
- Topic: Uroboros Residency
- Replies: 44
- Views: 42268
Re: Uroboros Residency
It looks great Less!! very impresive!!
- Sun Dec 16, 2007 9:55 am
- Forum: Kiln Casting
- Topic: Surface Issues
- Replies: 1
- Views: 7202
Re: Surface Issues
Luchooooo
You really have Sweet loving granny )
You really have Sweet loving granny )
- Fri Dec 14, 2007 12:17 pm
- Forum: Photos and Stuff
- Topic: New Panels
- Replies: 6
- Views: 10216
Re: New Panels
Dear Les
What a nice family u have
from so far away i can see the beauty of your land!
Through your work .. your stories.. the Rocky Mountain ..
I travell Canada with you:)
Thank u for sharing all this beauty
Oritt
What a nice family u have
from so far away i can see the beauty of your land!
Through your work .. your stories.. the Rocky Mountain ..
I travell Canada with you:)
Thank u for sharing all this beauty
Oritt