Search found 286 matches

by The Hobbyist
Sat Aug 27, 2022 9:44 am
Forum: Techniques and Tools
Topic: belts
Replies: 2
Views: 15702

Re: belts

I looked into this problem last year and found that the glue wound cost more than buying a replacement belt. I don't remember the product but I think I did a google.

Jim
by The Hobbyist
Mon Aug 15, 2022 9:49 am
Forum: Techniques and Tools
Topic: how to use this glass cutting tool?
Replies: 5
Views: 10347

Re: how to use this glass cutting tool?

My guess is that it is intended to score radii for an already scored circle. Thus enabling you to remove a circle from within a sheet of glass.

Jim

ps. I don't believe it's a toothbrush.
by The Hobbyist
Sun Apr 10, 2022 10:35 am
Forum: Techniques and Tools
Topic: Engraving signature on white fused glass art
Replies: 5
Views: 8227

Re: Engraving signature on white fused glass art

I have been using a pen and "ink" to sign my work for years, I tried a Dremel and diamond scriber and was terrible with both. As per Elskus, I mix Reusche black with clove oil to make "ink". A tiny jar lasts years. Use the "ink" and a simple nib pen to write whatever yo...
by The Hobbyist
Wed Oct 06, 2021 10:29 am
Forum: Techniques and Tools
Topic: The screw on running pliers.
Replies: 20
Views: 84472

Re: The screw on running pliers.

Throughout this discussion are you using breaking pliers with the customary plastic cushions on the jaw faces? It seems to me that if you are then they have a greater effect on the break than the screw. Uneven pressure is the cause of the flare and that pressure comes from the cushions as they touch...
by The Hobbyist
Thu Jul 15, 2021 9:19 am
Forum: Techniques and Tools
Topic: The screw on running pliers.
Replies: 20
Views: 84472

Re: The screw on running pliers.

So, how do you set the screw to the correct depth? It would seem to be a very narrow range between too tight and too loose since there is so little flex involved in breaking the score. It would also appear necessary to adjust it each time you break a new piece of glass, especially BE since the thick...
by The Hobbyist
Tue Dec 29, 2020 2:27 pm
Forum: Techniques and Tools
Topic: Scrap into sheet?
Replies: 8
Views: 15568

Re: Scrap into sheet?

Years ago I had the same thoughts you're experiencing. From them the "Hobbyist" lace technique was developed. When I was just starting in fused glass I acquired a few hundred pounds of clear BE scrap. I couldn't do any thing creative with the pieces so I started turning the scraps into fri...
by The Hobbyist
Fri Oct 02, 2020 9:36 am
Forum: Techniques and Tools
Topic: Kiln electrical question
Replies: 4
Views: 11057

Re: Kiln electrical question

I thought the fuse was to protect the wiring not the appliance. However, if the original setup was correct with a 60 amp fuse on a 4 awg wire then downgrading to a 45 amp fuse would be OK. But the reverse would be dangerous; replacing a 45 amp fuse on 6 awg wire with a 60 amp fuse. I suppose you cou...
by The Hobbyist
Mon Aug 31, 2020 8:54 am
Forum: Newcomer Forum
Topic: frit lace rescue
Replies: 5
Views: 17242

Re: frit lace rescue

Nice job...well done!

Jim "The Hobbyist"
by The Hobbyist
Wed Jan 08, 2020 9:24 am
Forum: Techniques and Tools
Topic: lace glass
Replies: 12
Views: 29606

Re: lace glass

I've always made lace on a primed shelf.

Maybe I'll try it on thinfire sometime. Please report your results if you try it.

Jim
by The Hobbyist
Fri Jul 12, 2019 10:59 am
Forum: Newcomer Forum
Topic: Round piece of glass.....sagging
Replies: 4
Views: 8162

Re: Round piece of glass.....sagging

The circle will sag like the square, by folding in a few places. If centered on the post it will end up with even height edges without the peaks you get with a square drape/sag.

Do a test with a circle of float to see if you get the effect you want.

Jim
by The Hobbyist
Tue May 21, 2019 9:56 am
Forum: Techniques and Tools
Topic: Drop Ring from thick slab
Replies: 11
Views: 19353

Re: Drop Ring from thick slab

I would be very worried that the whole thing will fall through the drop ring hole. You said the glass is 5.5" in diameter and the drop ring hole is 4". That only leaves 3/4" of glass on the edges and it also looks to be chipped out. I don't see how it can hold on. However, I hardly ev...
by The Hobbyist
Mon Apr 01, 2019 10:31 am
Forum: Techniques and Tools
Topic: float glass fusing problem - bends
Replies: 11
Views: 13327

Re: float glass fusing problem - bends

Looks like a clear case of incompatibility. Not all float glass is the same COE. You are using two different manufacturers which would most likely mean they are different glass formulas.

Jim "The Hobbyist"
by The Hobbyist
Sun Jan 13, 2019 10:08 am
Forum: Techniques and Tools
Topic: irritating news
Replies: 11
Views: 32614

Re: irritating news

Welcome back! I'm happy for you that you are, at least partially, rebuilt and newly functional.

Can we look forward to pictures and reports of your progress with your studio repair?

Jim "The Hobbyist"
by The Hobbyist
Sat Dec 22, 2018 9:02 am
Forum: Newcomer Forum
Topic: Galvanized Steel
Replies: 4
Views: 11797

Re: Galvanized Steel

Go to your local hardware and look at a piece of metal pipe. You should find black pipe and galvanized. Black pipe is just what it's called...black and usually oily/greasy to reduce rusting for a while. The galvanized will be silvery colored and not smooth. It is a dullish silver, not bright and shi...
by The Hobbyist
Fri Dec 14, 2018 10:21 am
Forum: Techniques and Tools
Topic: Removing sticker 'ghost marks'
Replies: 11
Views: 24733

Re: Removing sticker 'ghost marks'

Paint thinner and lacquer thinner are my favorites. Lighter fluid if you have it also is very good. Very high evaporative rate.

Jim "The Hobbyist"
by The Hobbyist
Mon Aug 13, 2018 10:55 am
Forum: Techniques and Tools
Topic: Alcohol ink and float glass
Replies: 3
Views: 8488

Re: Alcohol ink and float glass

Cover the surface with an even (or not) layer of powder that is compatible with float. When fired to full fuse it will "flow" into the cracks and give you the effect I think you're seeking. There is also a BE tip sheet on coating frit with powder in a container using water and then forming...
by The Hobbyist
Sun Jul 22, 2018 10:33 am
Forum: Techniques and Tools
Topic: firing schedule
Replies: 1
Views: 5921

Re: firing schedule

I would add/change 50 800 to the anneal for this one and the next.

Jim "The Hobbyist"
by The Hobbyist
Sat May 19, 2018 11:38 am
Forum: Techniques and Tools
Topic: Slumping Tempered Glass
Replies: 5
Views: 13940

Re: Slumping Tempered Glass

Sure, you can order exactly what you want/need but there are so many glass table tops floating around at great prices, new and used. Many of these are tempered and some are not. The savings are worth the effort if you can work with that glass. I just trashed a 5' = 60" diam x 3/4" glass to...
by The Hobbyist
Wed Apr 25, 2018 11:34 am
Forum: Photos and Stuff
Topic: Another...recent work
Replies: 9
Views: 18807

Re: Another...recent work

Nikki, what a pleasure to hear from you. You must have been on that sorting team also if you got one of my 3 x 5 "Thank You" cards. Those early magless exchanges were great and I still treasure them. For sure, you are welcome to visit in March, or any time. Although that's a long way off. ...
by The Hobbyist
Fri Mar 09, 2018 4:29 pm
Forum: Kiln Casting
Topic: Whiting as texture mold
Replies: 1
Views: 14754

Whiting as texture mold

Will a nice layer of whiting spread on the shelf with a texture pattern pressed into the surface serve as a mold for kilncarving? Or is it too soft? Can it be stiffened?

Jin "The Hobbyist"