Search found 237 matches
- Wed Aug 22, 2012 9:48 pm
- Forum: Techniques and Tools
- Topic: Frit Maker
- Replies: 11
- Views: 21418
Re: Frit Maker
garbage disposal works for me. Depends on the size of the frit you want, and you do have to wash it but it's a heck of a lot faster than the quench method.
- Sun Jul 22, 2012 9:39 pm
- Forum: Techniques and Tools
- Topic: Menorah candle cups
- Replies: 2
- Views: 4304
Re: Menorah candle cups
1. get the cups first. Weiss is a good source. There aren't that many that I've found. 2. THEN figure out how to attach. Without the cups, you won't know if they've got a hole or not. Threaded rods are just screws without tops. You can buy them at Home Depot in the bin with the long metal stuff. Som...
- Mon Jul 09, 2012 9:21 pm
- Forum: Techniques and Tools
- Topic: Where can I find this?
- Replies: 12
- Views: 11039
Re: Where can I find this?
Have you tried contacting the artist whose work you posted?
- Mon Jul 09, 2012 9:15 pm
- Forum: Newcomer Forum
- Topic: Fiber floor kiln
- Replies: 13
- Views: 14742
Re: Fiber floor kiln
ok, now that we all know to elevate the shelf... Figuring out firing schedules for a new kiln takes time. I have 7 (yes, seven) kilns and each one of them fires differently (even 2 of the same kiln...). So stop pulling your hair out (unless it grows back very quickly) and fire some test pieces rathe...
- Mon Jul 09, 2012 2:27 pm
- Forum: Business Topics
- Topic: Art 101 Gallery in Wooster/Medina Ohio?
- Replies: 5
- Views: 8841
Re: Art 101 Gallery in Wooster/Medina Ohio?
i heard from some other artists and you are right! How are you my friend?
- Sun Jul 08, 2012 9:16 pm
- Forum: Business Topics
- Topic: Art 101 Gallery in Wooster/Medina Ohio?
- Replies: 5
- Views: 8841
Art 101 Gallery in Wooster/Medina Ohio?
I was just contacted by this gallery. After checking out their web site, they appear to have 1 glass artist who does not have a web site. Has anyone dealt with or heard of these folks? They sound a little scammy to me...
thanks!
thanks!
- Fri Jul 06, 2012 9:55 pm
- Forum: Techniques and Tools
- Topic: how to flatten and fp pot melt
- Replies: 2
- Views: 4115
Re: how to flatten and fp pot melt
Flattening takes a much hotter temperature than firepolishing. If you want to flatten and not lose the rectangular shape, use a dam. If you do that, the top will be firepolished but not the sides (where they're touching the dam.
- Fri Jul 06, 2012 9:54 pm
- Forum: Techniques and Tools
- Topic: Pressing glass into a mold?
- Replies: 5
- Views: 7392
Re: Pressing glass into a mold?
check out www.fusedglass.org and take a look at Paul Tarlow's process for Kiln-Pressed Glass. Could be just the ticket for getting the maximum purple out of that glass!
- Fri Jul 06, 2012 9:51 pm
- Forum: Newcomer Forum
- Topic: Screen Melts
- Replies: 9
- Views: 11717
Re: Screen Melts
Don't hesitate to re-use your shattered pieces in new melts/pieces. That's part of the joy of fusing!
- Fri Apr 16, 2004 6:19 pm
- Forum: Business Topics
- Topic: Urban Glass-Glassblower's Ball & Auction
- Replies: 6
- Views: 10876
silent, indeed!
Marty!!!!! (actually you can check out Marty on his Web site, but I prefer the pup...)
- Thu Apr 15, 2004 1:55 pm
- Forum: Photos and Stuff
- Topic: Someone please tell me how the heck to post photos
- Replies: 23
- Views: 34173
interesting...
I went thru a one-day critique recently with Steve Klein and asked that very question - about adding almost a border (like a quilt) between the work and the frame. Folks said no, but I'm still tinkering with the idea. Interesting that you brought it up.
- Wed Apr 14, 2004 10:37 am
- Forum: Business Topics
- Topic: Art Glass Network
- Replies: 2
- Views: 6512
Art Glass Network
I just bumped into the Art Glass Network, http://www.artglassnetwork.com. Anyone know anything? They seem to have some relatively well-known folks listed as selling on the site...
- Tue Apr 13, 2004 5:23 pm
- Forum: Kiln Casting
- Topic: Sand casting question
- Replies: 13
- Views: 22605
raku tongs work
and they're cheaper too
- Tue Apr 13, 2004 5:20 pm
- Forum: Photos and Stuff
- Topic: Someone please tell me how the heck to post photos
- Replies: 23
- Views: 34173
and bert...
it's personal! answer my email, you goon!!
- Tue Apr 13, 2004 5:19 pm
- Forum: Photos and Stuff
- Topic: Someone please tell me how the heck to post photos
- Replies: 23
- Views: 34173
hanging system
Arakawa - in Oregon. You can find them on the web, http://www.arakawagrip.com. Not cheap but good stuff.
- Tue Apr 13, 2004 11:35 am
- Forum: Photos and Stuff
- Topic: Someone please tell me how the heck to post photos
- Replies: 23
- Views: 34173
I'm stuck
can't seem to figure out how to set it to public (which I did at the beginning anyway). oh well.
- Tue Apr 13, 2004 10:13 am
- Forum: Photos and Stuff
- Topic: Someone please tell me how the heck to post photos
- Replies: 23
- Views: 34173
- Mon Apr 12, 2004 6:13 pm
- Forum: Photos and Stuff
- Topic: Someone please tell me how the heck to post photos
- Replies: 23
- Views: 34173
Someone please tell me how the heck to post photos
who's the moderator here, anyway? Where's the FAQ? I'm so low-tech, I might as well be NO-tech...
- Thu Mar 11, 2004 8:31 pm
- Forum: Techniques and Tools
- Topic: WGW 2004?
- Replies: 40
- Views: 51384
me 2
Just got the most recent GAS newsletter, reading the conference stuff, even the pre & post workshops are 99% blowing. I've said it before, and I'll say it again: we need a group.
Besides, couldn't we require all members to buy a calendar? It's definitely a collector's item
Besides, couldn't we require all members to buy a calendar? It's definitely a collector's item
- Tue Mar 09, 2004 6:27 pm
- Forum: Techniques and Tools
- Topic: drip lines - how hot?
- Replies: 10
- Views: 11079
and...
wonder if I could use vermiculite board??? a bit sturdier....