by grammy
Tue Jun 27, 2017 8:11 pm
Forum: Photos and Stuff
Topic: As promised...a recent work
Replies: 4
Views: 5731

Re: As promised...a recent work

Sweet Jim
by grammy
Sat Jan 28, 2017 7:26 pm
Forum: Techniques and Tools
Topic: Annealing Question
Replies: 3
Views: 4573

Annealing Question

I am getting back into fusing glass. I have some small jewelry sized piesces that are double thick fully fused. I am now adding a decal to these pieces. These are low heat 24kt gold decals that say go to 1100. Do I have to anneal these? Just wondering if I can get by without it.

Thanks
by grammy
Sat Jan 07, 2017 5:18 pm
Forum: Business Topics
Topic: Forgot Studio Name
Replies: 4
Views: 6215

Re: Forgot Studio Name

I am sad that they closed but happy for them to retire and enjoy other things, like teaching more. I now live in NC which Warm Glass is a lot closer. I ws working on a resume of where I had taken classes and could not remember then names. Judith Conway and Kevin ...... I have it down somewhere. Than...
by grammy
Fri Jan 06, 2017 3:10 pm
Forum: Business Topics
Topic: Forgot Studio Name
Replies: 4
Views: 6215

Re: Forgot Studio Name

Thanks
by grammy
Fri Dec 30, 2016 11:57 am
Forum: Business Topics
Topic: Forgot Studio Name
Replies: 4
Views: 6215

Forgot Studio Name

I have taken a class in Laurel MD and can not remember the name of the studio or the teachers. O'Toole? Can anyone help? They are closing their doors soon.
by grammy
Sat Nov 26, 2016 12:15 pm
Forum: Newcomer Forum
Topic: Texture Tile Question
Replies: 6
Views: 7311

Re: Texture Tile Question

Even though you have fully fused your blank, you would still go to a contour fuse. For my kiln I would go slightly higher, maybe 20 degrees as the glass has to get soft enough to flow into the contour. I would not put any holes in the mold itself.
by grammy
Thu Sep 08, 2016 4:24 pm
Forum: Techniques and Tools
Topic: Silver Foil
Replies: 7
Views: 6110

Re: Silver Foil

Where do you get silver foil? I went to Michaels and that did not look like real silver to me. :shock:
by grammy
Tue May 24, 2016 11:51 am
Forum: Community Projects
Topic: 2016 Magless Exchange
Replies: 20
Views: 34414

Re: 2016 Magless Exchange

KaCee are you ready to post pictures?
by grammy
Tue May 24, 2016 11:46 am
Forum: Techniques and Tools
Topic: Devit Spray and Dichoric
Replies: 4
Views: 4811

Re: Devit Spray and Dichoric

Thanks for the reply. I am going to try it later. My art show is over and I am going to relax for a little.
by grammy
Sat May 14, 2016 9:29 pm
Forum: Techniques and Tools
Topic: Devit Spray and Dichoric
Replies: 4
Views: 4811

Devit Spray and Dichoric

I am making projects that seem to be getting devit on the second firing. These pieces will have dichroic on the top and tack fused. Will the clear coating affect the dichroic? TIA
by grammy
Sun May 01, 2016 11:22 am
Forum: Photos and Stuff
Topic: Eyesore#3 and Eyesore#4
Replies: 1
Views: 3697

Re: Eyesore#3 and Eyesore#4

I love the flow of #4. Great job.
by grammy
Wed Apr 27, 2016 6:51 am
Forum: Techniques and Tools
Topic: Lesson Learned - Major Devit
Replies: 0
Views: 4149

Lesson Learned - Major Devit

I was in a hurry to make some discs for garden stakes. So I put a 10" one on a shelf and then decided to put a shelf above it with a 12" disc. Well, there was very ventilation for the bottom glass so I got major devit. Lesson learned. Now to get that stuff off. Since I do not have a sand b...
by grammy
Mon Mar 28, 2016 8:05 pm
Forum: Techniques and Tools
Topic: Best Glue for Garden Stakes
Replies: 7
Views: 6901

Re: Best Glue for Garden Stakes

Thanks. I did not find the Loctite that was mentioned but got an epoxy for metal to glass.
by grammy
Fri Mar 25, 2016 9:43 pm
Forum: Techniques and Tools
Topic: Best Glue for Garden Stakes
Replies: 7
Views: 6901

Re: Best Glue for Garden Stakes

Thank you.
by grammy
Fri Mar 25, 2016 10:45 am
Forum: Techniques and Tools
Topic: Best Glue for Garden Stakes
Replies: 7
Views: 6901

Best Glue for Garden Stakes

I am replacing some glass for a client in their garden stakes. So these will be outside. The stakes do not have a way to "clip" in the glass, only glueing to the metal. What glue would be best? E6000?
by grammy
Thu Feb 18, 2016 7:41 pm
Forum: Community Projects
Topic: 2016 Magless Exchange
Replies: 20
Views: 34414

Re: 2016 Magless Exchange

Debbie Shank aka Grammy. dennisanddebbieshank@gmail.com
by grammy
Fri Jan 22, 2016 6:35 pm
Forum: Community Projects
Topic: No more Magless Exchange?
Replies: 12
Views: 17015

Re: No more Magless Exchange?

I've never participated in the Mag Exchange but would like to if you pull it together. I am a true novice when it comes to design but can have fun.
by grammy
Wed Dec 23, 2015 11:37 am
Forum: Techniques and Tools
Topic: Boiling Glass?
Replies: 9
Views: 13284

Boiling Glass?

I have seen several references on You Tube about boiling glass. It is where you put a layer of glass down, then bubble powder, then two more layers of glass. Take it to 1700 and and the bubbles rise and mix the glass. My thought is that it does not exactly "boil" is that so? I was wonderin...
by grammy
Thu Dec 03, 2015 2:11 pm
Forum: Newcomer Forum
Topic: Kiln wash
Replies: 5
Views: 6307

Re: Kiln wash

I use a dry wall sander on mine. It get the wash off really fast.
by grammy
Mon Nov 23, 2015 9:44 pm
Forum: Photos and Stuff
Topic: Blowing OUT large Colour bar sections
Replies: 28
Views: 29867

Re: Blowing OUT large Colour bar sections

Absolutely beautiful. I am always fascinated by your work.