- Mon Jul 15, 2013 3:02 pm
- Forum: Newcomer Forum
- Topic: Help With a Piece Breaking
- Replies: 6
- Views: 16613
Re: Help With a Piece Breaking
Thank you Stephen. I will try doing it differently and making some adjustments to the schedule. I really appreciate everyone's help!
- Mon Jul 15, 2013 2:30 pm
- Forum: Newcomer Forum
- Topic: Help With a Piece Breaking
- Replies: 6
- Views: 16613
Re: Help With a Piece Breaking
Thanks for the reply. The 1250 with the hold did tack them together. Maybe not enough? The problem wasn't that they came loose, but that they actually snapped right in half. That's why I thought it was annealing, because it's right where the 2 pieces meet. That leads me to more questions. Would the ...
- Mon Jul 15, 2013 12:55 pm
- Forum: Newcomer Forum
- Topic: Help With a Piece Breaking
- Replies: 6
- Views: 16613
Help With a Piece Breaking
Hello All, I was hoping someone could help me out with a problem I'm having. My mom wanted me to make her some little thinks to stick in her garden. I was just going to do simple little flower type things, kind of like Spectrum's "Spirit Flakes" that they have on their site. I took two tri...
- Tue Oct 09, 2012 9:17 am
- Forum: Newcomer Forum
- Topic: Lettering
- Replies: 20
- Views: 60243
Re: Lettering
Thank you all so much for the ideas. Still not sure how I am going to tackle it, but I definitely have a ton of methods to look into. Really appreciate the help! 
- Mon Oct 08, 2012 10:07 am
- Forum: Newcomer Forum
- Topic: Lettering
- Replies: 20
- Views: 60243
Lettering
I have a friend that would like her company name put on a plate. I am trying to figure out the best way to attack the lettering. Does anyone have any ideas they are willing to share? I was thinking of using frit and "drawing" it on using something like Liquid Stringer. The other option I h...
- Tue Sep 25, 2012 11:50 am
- Forum: Newcomer Forum
- Topic: Bubble or "Tumor" Forming During Slump
- Replies: 11
- Views: 29449
Re: Bubble or "Tumor" Forming During Slump
Thanks, I'll try that. 
- Sun Sep 23, 2012 8:09 pm
- Forum: Newcomer Forum
- Topic: Bubble or "Tumor" Forming During Slump
- Replies: 11
- Views: 29449
Re: Bubble or "Tumor" Forming During Slump
Thanks. I've never drilled a hole in a ceramic mold before. Do I need a special bit? Does it have to be wet or anything like glass does?
- Sat Sep 22, 2012 6:34 pm
- Forum: Newcomer Forum
- Topic: Bubble or "Tumor" Forming During Slump
- Replies: 11
- Views: 29449
Re: Bubble or "Tumor" Forming During Slump
I don't have a pic of the slump handy. I can post it later. The mold is this one... http://www.delphiglass.com/glass-molds/plates-platter-molds/10-rimmed-dinner-plate It has a single hole in the bottom. My first thought would normallybe the hole, but why would it have worked for the last 4 years or ...
- Sat Sep 22, 2012 11:19 am
- Forum: Newcomer Forum
- Topic: Bubble or "Tumor" Forming During Slump
- Replies: 11
- Views: 29449
Re: Bubble or "Tumor" Forming During Slump
Thanks Vernelle.
I have put the 10 plate mold onto small kiln posts to make sure it has air circulation and that the hole in the bottom is completely clear.
I have put the 10 plate mold onto small kiln posts to make sure it has air circulation and that the hole in the bottom is completely clear.
- Sat Sep 22, 2012 10:25 am
- Forum: Newcomer Forum
- Topic: Bubble or "Tumor" Forming During Slump
- Replies: 11
- Views: 29449
Bubble or "Tumor" Forming During Slump
Good Morning All, I am having an issue that I just cannot seem to correct. I've tried every variation I can think of, and nothing seems to be working. Here's the issue. I am taking a fully fused "blank" (Spectrum black with clear cap, fully fused, no problems) and putting it in your averag...