Search found 158 matches

by AndyT
Mon Mar 04, 2024 1:04 pm
Forum: Techniques and Tools
Topic: oceanside QC
Replies: 5
Views: 13402

Re: oceanside QC

The prices of OGT have continued to rise to the point that they are now competitive with BE, KOK and others. I think they've become better at making the colors more vibrant. I've never had a bad experience with OGT for fusing. Hi Bob. Have you read the posts and opinions on OC from Craftweb? The bul...
by AndyT
Fri Nov 24, 2023 12:46 pm
Forum: Techniques and Tools
Topic: Tile saw blade
Replies: 2
Views: 18385

Re: Tile saw blade

I bought my blade at Home Depot. DeWalt Glass Tile Blade. About $24. Used it to cut 100's of bottles and slags.
by AndyT
Sat Nov 18, 2023 12:51 pm
Forum: Techniques and Tools
Topic: Alternative to Thinfire
Replies: 22
Views: 137681

Re: Alternative to Thinfire

The thing I like about Papyros is that if you're careful you can get several firings on it. I've gotten up to five. Often it depends on the color of the glass and how hot you go.
by AndyT
Sat Mar 18, 2023 12:00 pm
Forum: Newcomer Forum
Topic: Hotline Glass
Replies: 1
Views: 13415

Re: Hotline Glass

Hello I have been given some Hotline glass stringers with a catalog number 4955, 4954 and Millefiori slices number 1554. Can anyone help with the COE of these? Thanks Karen Layton The Mille is 104. The stringers could be 90 or 96. Hotline products are from Creative Craftsman. https://gofusing.com/b...
by AndyT
Fri Aug 26, 2022 7:34 pm
Forum: Newcomer Forum
Topic: A-14?
Replies: 6
Views: 23455

Re: A-14?

Don Burt wrote:A13 Is an acrylic medium from Thompson Enamel. There. Thats infinitely helpful, isn't it?
I thought it was a Bingo number....
by AndyT
Wed Mar 16, 2022 3:45 pm
Forum: Techniques and Tools
Topic: How is thin fire made?
Replies: 0
Views: 100524

How is thin fire made?

Does anyone know the process in which thin fire paper or Papyros is made? Looking for more info other than it's just impregnated with a ceramic material. Thanks!
by AndyT
Mon Feb 21, 2022 8:09 pm
Forum: Techniques and Tools
Topic: Moving a compressor. Disassemble?
Replies: 10
Views: 21413

Re: Moving a compressor. Disassemble?

Drain the oil and take it apart. Here's a good link. https://www.garagejournal.com/forum/thr ... sor.28198/
by AndyT
Sat Dec 04, 2021 1:19 pm
Forum: Techniques and Tools
Topic: Shrinkage during fusing attemp
Replies: 3
Views: 7362

Re: Shrinkage during fusing attemp

You would need to have them at least overlap or better yet on a clear base.
by AndyT
Mon Sep 27, 2021 12:11 pm
Forum: Techniques and Tools
Topic: Drill bit attachment
Replies: 8
Views: 9480

Re: Drill bit attachment

Because this is smoothing down the side of 1/4" flat glass, I want it to be super easy for the client. That is why I am sending her a 1" diameter Aanraku grinding bit. Easier to control than a smaller bit. I am suggesting someone spray water on the glass as she grinds it down. (I will mak...
by AndyT
Sun Sep 26, 2021 11:57 am
Forum: Techniques and Tools
Topic: Drill bit attachment
Replies: 8
Views: 9480

Re: Drill bit attachment

You'd need a small steel rod with a flat side. The rod would go into the bit and then the allen screw would be used to tighten the bit to the rod. You could just find a diamond bit that is designed to fit in a drill. https://www.harborfreight.com/diamond-rotary-bit-set-4-pc-69664.html?utm_source=goo...
by AndyT
Fri Sep 03, 2021 8:25 pm
Forum: Techniques and Tools
Topic: The screw on running pliers.
Replies: 20
Views: 84454

Re: The screw on running pliers.

I've never used the screw in 40 years and I've cut all sorts of glass. I just take the screw out and throw it into the trash.
by AndyT
Fri Aug 13, 2021 12:05 pm
Forum: Techniques and Tools
Topic: Tiny Hole Saw Bits for a Dremel?
Replies: 13
Views: 26579

Re: Tiny Hole Saw Bits for a Dremel?

Google "Tiny diamond drill bits" Several sources out there.
by AndyT
Wed Jul 21, 2021 12:14 pm
Forum: Newcomer Forum
Topic: Suggestions for storing stringers and rods
Replies: 1
Views: 19446

Re: Suggestions for storing stringers and rods

Different sizes of PVC pipe. In my last store, I had many different sizes as well as different lengths.
by AndyT
Mon Jul 12, 2021 2:40 pm
Forum: Techniques and Tools
Topic: 1/4 inch jaw running pliers
Replies: 13
Views: 14962

Re: 1/4 inch jaw running pliers

Glastar makes a narrow running plier. https://www.amazon.com/Unknown-Glastar- ... B004KHYG6I
by AndyT
Thu Jan 21, 2021 1:29 pm
Forum: Newcomer Forum
Topic: Paragon Kiln Help
Replies: 2
Views: 23988

Re: Paragon Kiln Help

Find Arnold Howard on FB. He was the kiln guy at Paragon and is now working on kilns on his own. https://www.facebook.com/arnoldhoward
by AndyT
Thu Aug 06, 2020 12:06 pm
Forum: Techniques and Tools
Topic: Denver kiln
Replies: 6
Views: 8922

Re: Denver kiln

I'd go with a Skutt or Olympic.
by AndyT
Tue Mar 10, 2020 11:49 am
Forum: Newcomer Forum
Topic: Iowa resources & some kiln supply & ring sawn questions
Replies: 2
Views: 12082

Re: Iowa resources & some kiln supply & ring sawn questions

As for your T3....most likely the belt is bad. Stretched and just old. It's one of the most common parts to go bad and cause the blade to keep slipping off.
by AndyT
Fri Feb 14, 2020 6:13 pm
Forum: Photos and Stuff
Topic: new work
Replies: 15
Views: 50844

Re: new work

If anyone can tell me what I did wrong, let me know. I went to attachments, and added a file. It showed the file at the bottom but when I preview, all I see is my text. Tried drag/drop as well with the same result. Is there a size issue? Save the pic to your desktop and make it a jpeg. then click t...