Damming inch thick large rounds
I'm going to fuse inch thick (three layers) and 18 inches in diameter float glass rounds and am wondering if anyone has suggestions for the best damming materials? I've used thin fire strips backed by eighth inch blanket strips and then contained it with a stainless hose clamp band, but the glass ed...