Re: Heat resistant Tape

@ Brad Walker: Instead of Ceramic felt between RVS and the glass. I saw somebody use it on Internet. For Full fuse . Jan
by Jan de Jong
Thu Apr 08, 2021 9:28 am
Forum: Techniques and Tools
Topic: Heat resistant Tape
Replies: 3
Views: 8467

Heat resistant Tape

Hallo, did see on a site heatresistant tape which was used by fusing. I marked the site as Favorite to look on it later.
Something went wrong.....no favorite and no idea where to search.
So my question is: is there tape with which you can fuse ?
Jan
by Jan de Jong
Thu Apr 08, 2021 5:40 am
Forum: Newcomer Forum
Topic: Heatresistent Tape
Replies: 2
Views: 23245

Re: Heatresistent Tape

@ Buttercup: Thank you for your info. Yes, I found already more of this tape, but I doubt if it is fuseble. So I hope somebody know a better tape :) Jan de Jong
by Jan de Jong
Fri Apr 02, 2021 1:02 pm
Forum: Newcomer Forum
Topic: Heatresistent Tape
Replies: 2
Views: 23245

Heatresistent Tape

Hello, A few weeks ago I saw on a site for Fusing the use of heatresistent Tape. I thought that I had the site as Favorite to see it later. It's a pity.....not in the Favorites and by searching....I can find nothing for this tape ? Somebody a suggestion ? Jan de Jong (Holland)
by Jan de Jong
Tue Jan 05, 2021 4:45 am
Forum: Newcomer Forum
Topic: White spirit
Replies: 10
Views: 36926

Re: White spirit

@ Buttercup: Thank you so much for your answers !!
I go reading your suggestions and see what I can use.Jan
by Jan de Jong
Mon Jan 04, 2021 7:13 am
Forum: Newcomer Forum
Topic: White spirit
Replies: 10
Views: 36926

Re: White spirit

@ Buttercup: Thanks ! I did ask for White Spirit and Turpentine, but I had better first look at the label on the Revell Email Paint ....I become afraid when I read that: Danger. Contains Hydrocarbons, C9-C11, n-alkanes, isoalkanes cyclics, 2% aromatics, 1-methoxypropan-2-pf phtalic, anhydride. Flamm...
by Jan de Jong
Sun Jan 03, 2021 5:53 am
Forum: Newcomer Forum
Topic: White spirit
Replies: 10
Views: 36926

Re: White spirit

@ buttercup: Thank you for this information. Please can you tell me if I can use Turpentine and fire in the kiln ? Jan
by Jan de Jong
Sat Jan 02, 2021 4:54 pm
Forum: Newcomer Forum
Topic: White spirit
Replies: 10
Views: 36926

Re: White spirit

@ Jim simmons: you make it difficult for me. Difficult die me to write in English language. I found in English Wikipedia What White Spirit is. In Holland we call it Terpentine.....in English Turpentine (?)
Can I fire this in my kiln ?? Jan
by Jan de Jong
Fri Jan 01, 2021 10:00 am
Forum: Newcomer Forum
Topic: White spirit
Replies: 10
Views: 36926

White spirit

I have some enamel paint which must be dissolved with White Spirit. When doing this ...is firing in a kiln still possible ?? Jan
by Jan de Jong
Mon Nov 23, 2020 1:40 pm
Forum: Newcomer Forum
Topic: BE opaline strike temp
Replies: 1
Views: 23700

Re: BE opaline strike temp

Jim, no answers so I decided to try to help you but I am not sure you mean this! Bullseye site: Opaline striker....Full fuse. Jan
by Jan de Jong
Sun Nov 22, 2020 4:00 pm
Forum: Newcomer Forum
Topic: Drop with Dropring
Replies: 16
Views: 49224

Re: Drop with Dropring

Hello, with your help I was able to make a good drop, but this was with only blank and transparent glass. Now I wish to make a new drop with opal glass and then a good design is a must. Michaelmace wrote: " You asked what will happen to the layers. The layer of glass on the bottom (closest to t...
by Jan de Jong
Sat Nov 07, 2020 12:23 pm
Forum: Newcomer Forum
Topic: Reading COE
Replies: 2
Views: 23698

Re: Reading COE

@ Lynn Perry: Thank you ! Jan
by Jan de Jong
Sat Nov 07, 2020 10:06 am
Forum: Newcomer Forum
Topic: Reading COE
Replies: 2
Views: 23698

Reading COE

Hello, not knowing about this notation of COE. I think it is COE 96 ....am I right ?
COE (9,60 +- 0,15) x 10 -6 Sorry, don 't know how to make this signs in the right way. Jan
by Jan de Jong
Tue Nov 03, 2020 11:00 am
Forum: Newcomer Forum
Topic: Boron Nitride POWDER
Replies: 4
Views: 26285

Re: Boron Nitride POWDER

@ Jim: Thank you ! I PM you for another question. Jan
by Jan de Jong
Mon Nov 02, 2020 9:38 am
Forum: Newcomer Forum
Topic: Boron Nitride POWDER
Replies: 4
Views: 26285

Re: Boron Nitride POWDER

@ Jim Simmons: Thank you for your reply !! Do you heat the SS ( and Clay fired) ?? Jan
by Jan de Jong
Sat Oct 31, 2020 1:20 pm
Forum: Newcomer Forum
Topic: Boron Nitride POWDER
Replies: 4
Views: 26285

Boron Nitride POWDER

I found this question here from long ago, but there was no response.
Boron Nitride spray is used as seperator on RVS.
But there is also POWDER. Had anyone try this ?? Jan
by Jan de Jong
Mon Oct 26, 2020 1:43 pm
Forum: Newcomer Forum
Topic: Drop with Dropring
Replies: 16
Views: 49224

Re: Drop with Dropring

Sorry for late respons. Thank you Michael Stevens and michaelmace ! In the past there was a notification when there was a new mail, but now not anymore (or have I done something wrong ?) Jan
by Jan de Jong
Thu Aug 06, 2020 3:33 am
Forum: Newcomer Forum
Topic: Drop with Dropring
Replies: 16
Views: 49224

Re: Drop with Dropring

@ Kevin: Okay, I go for 4 layers and see what happens :wink: Jan
by Jan de Jong
Wed Aug 05, 2020 4:34 am
Forum: Newcomer Forum
Topic: Drop with Dropring
Replies: 16
Views: 49224

Re: Drop with Dropring

After posting I was thinking: what happens by 5 layers ? Will these be visible ? Jan
by Jan de Jong
Wed Aug 05, 2020 4:27 am
Forum: Newcomer Forum
Topic: Drop with Dropring
Replies: 16
Views: 49224

Re: Drop with Dropring

For help to others: Like to share the link I found: https://www.warmtips.com/20060303.htm Jan