Search found 68 matches
- Sun Jun 21, 2015 12:36 pm
- Forum: Techniques and Tools
- Topic: spray kiln shelf
- Replies: 6
- Views: 12028
spray kiln shelf
Is it effective to spray kiln on a shelf using a simple household spray bottle - one you'd use to spray water on plants? I'm going to fire irid face down and want to be sure the kiln washed surface is in good shape. I've also read about the pros and cons of using thin fire when firing irid face down...
- Wed Feb 11, 2015 12:17 am
- Forum: Techniques and Tools
- Topic: Joining up stringers
- Replies: 16
- Views: 18884
Re: Joining up stringers
Thanks Valerie
I thought that might be the best solution as I struggled with the stringers tonight
Susan
I thought that might be the best solution as I struggled with the stringers tonight
Susan
- Tue Feb 10, 2015 8:39 pm
- Forum: Techniques and Tools
- Topic: Joining up stringers
- Replies: 16
- Views: 18884
Re: Joining up stringers
If someone could give me some additional tips for cutting 2mm stringers, I'd be grateful. Doing my best to follow Cynthia's advice but I cannot seem to cut the stringers so they are all the same length. The piece I am working on has a base of two 2 mm pieces of tekta, with a design consisting of 2mm...
- Sun Dec 28, 2014 4:20 pm
- Forum: Art, philosophy, and content
- Topic: Silence
- Replies: 26
- Views: 96310
Re: Silence
I love this forum too
While I've not had much time for fusing in many months due to busy work schedule and family responsibilities, I frequently read this forum and love the way it keeps fused glass alive for me
Thank you to all
Susan
While I've not had much time for fusing in many months due to busy work schedule and family responsibilities, I frequently read this forum and love the way it keeps fused glass alive for me
Thank you to all
Susan
- Sun Dec 28, 2014 4:12 pm
- Forum: Newcomer Forum
- Topic: Sand corner of mold?
- Replies: 1
- Views: 4497
Sand corner of mold?
Happy holidays to all Finally have time to get back into my studio and I noticed a couple of the corners on BE molds are deteriorating slightly. Would you recommend sanding them a bit to even it out and then reapplying kiln wash ? Can I reapply kiln wash just to those spots or should I reapply it to...
- Sun Aug 31, 2014 10:32 pm
- Forum: Business Topics
- Topic: Designing a new studio
- Replies: 38
- Views: 61954
Re: Designing a new studio
No studio suggestions Marty
But I'd like to be one of those 10 students
Susan
But I'd like to be one of those 10 students
Susan
- Thu Mar 13, 2014 8:09 pm
- Forum: Community Projects
- Topic: Mailing magnets
- Replies: 8
- Views: 38554
Re: Mailing magnets
Thanks Charlie& Dana
- Wed Mar 12, 2014 6:26 pm
- Forum: Community Projects
- Topic: Mailing magnets
- Replies: 8
- Views: 38554
Re: Mailing magnets
Dana
Can you give me your source for the small bags? I can't find small ones in small quantities. Thanks
Susan
Can you give me your source for the small bags? I can't find small ones in small quantities. Thanks
Susan
- Mon Mar 10, 2014 9:39 pm
- Forum: Community Projects
- Topic: Mailing magnets
- Replies: 8
- Views: 38554
Mailing magnets
Ok...magnets done...any suggestions on best way to send them? Does each one need to be individually wrapped to be safely mailed? Thanks for the advice
Susan
Susan
- Sun Feb 23, 2014 9:36 pm
- Forum: Techniques and Tools
- Topic: Kickstarter molds
- Replies: 8
- Views: 11028
Re: Kickstarter molds
My molds came too
Thanks, Brad
Excited to try them out
Where on your site are the directions?
Thanks, Brad
Excited to try them out
Where on your site are the directions?
- Tue Feb 18, 2014 8:36 am
- Forum: Techniques and Tools
- Topic: kiln replacement
- Replies: 13
- Views: 16198
Re: kiln replacement
Thanks
I'll try bowing down after I close the lid
I'll try bowing down after I close the lid
- Mon Feb 17, 2014 9:33 pm
- Forum: Techniques and Tools
- Topic: kiln replacement
- Replies: 13
- Views: 16198
Re: kiln replacement
Valerie and others,
What kind of general maintenance do you suggest for a kiln?
I vacuum the elements and inside
What else?
Thanks
Susan
What kind of general maintenance do you suggest for a kiln?
I vacuum the elements and inside
What else?
Thanks
Susan
- Thu Jan 02, 2014 10:14 am
- Forum: Techniques and Tools
- Topic: kiln in unheated garage
- Replies: 9
- Views: 11859
Re: kiln in unheated garage
Rosanna
Do you think the controller could break due to the cold? I wouldn't want to chance it.
i have a small space heater... could use as you suggested
thanks for the advice
Do you think the controller could break due to the cold? I wouldn't want to chance it.
i have a small space heater... could use as you suggested
thanks for the advice
- Thu Jan 02, 2014 10:05 am
- Forum: Techniques and Tools
- Topic: kiln in unheated garage
- Replies: 9
- Views: 11859
kiln in unheated garage
Hi My kiln is in an unheated attached garage. I've never had problems firing it during the winter....but it has never been this cold since I've lived in this house. Temps in the mid hudson valley of NY will be below zero at night and single digits during the day. Does anyone think there are issues I...
- Wed Jan 01, 2014 8:48 pm
- Forum: Techniques and Tools
- Topic: Glue for fused work
- Replies: 24
- Views: 42486
Re: Glue for fused work
cheap liquid pump hairspray - currently using suave
i put it in a small bottle & use it with an eye dropper
i put it in a small bottle & use it with an eye dropper
- Wed Dec 18, 2013 9:56 pm
- Forum: Newcomer Forum
- Topic: Help putting frit in mold
- Replies: 5
- Views: 7529
Re: Help putting frit in mold
Shelley
I've thought about doing this too
what kind of molds are you using?
Susan
I've thought about doing this too
what kind of molds are you using?
Susan
- Tue Dec 17, 2013 9:07 pm
- Forum: Techniques and Tools
- Topic: Devit Problem with BE
- Replies: 21
- Views: 32157
Re: Devit Problem with BE
why?I keep the plug out of the peephole the entire process.
Susan
- Sun Jul 28, 2013 10:01 pm
- Forum: Photos and Stuff
- Topic: Taking photos
- Replies: 7
- Views: 10792
Re: Taking photos
Thanks for the replies & information.
Great reference website, Marty
Thanks Mike for the Idea of editing in photoshop. it did not occur to me but I think should solve most of my problems.
Risa....my spouse is also a photographer. He'll do the photoshop work for me.
Great reference website, Marty
Thanks Mike for the Idea of editing in photoshop. it did not occur to me but I think should solve most of my problems.
Risa....my spouse is also a photographer. He'll do the photoshop work for me.
- Sat Jul 27, 2013 1:05 pm
- Forum: Photos and Stuff
- Topic: Taking photos
- Replies: 7
- Views: 10792
Taking photos
I could use some help. I have a difficult time taking good pictures of my plates & bowls. No fancy camera....using either my cell phone or iPad. Any suggestions for better pictures? I've put pieces on a light box, but that distorts the colors. Also tried putting the pieces on a while piece of pa...
- Sun Jul 14, 2013 5:52 am
- Forum: Board Help
- Topic: Flagging a topic for easy retrieval later
- Replies: 4
- Views: 32065
Re: Flagging a topic for easy retrieval later
Thanks, Brad.
I've been emailing the topics to myself & now have quite a collection.
What an easier way to do this.
Susan
I've been emailing the topics to myself & now have quite a collection.
What an easier way to do this.
Susan