Realize that plaster/silica is not happy at any temps above 1400. 1675 is way above 1400. There are reasons people spend big bucks to cast with Gaffer glass or Schott. The lead lowers the maturing temps making for more reliable castings. hi Bert. my question is a bit off topic. i use a dry 50/50 mi...
- Mon Mar 15, 2004 10:55 pm
- Forum: Techniques and Tools
- Topic: Floatglass Break Help
- Replies: 7
- Views: 7932
- Fri Mar 05, 2004 9:17 pm
- Forum: Techniques and Tools
- Topic: Tried and tested sand casting mold question
- Replies: 7
- Views: 8127
- Thu Feb 19, 2004 11:24 pm
- Forum: Techniques and Tools
- Topic: newbie float question
- Replies: 13
- Views: 15717
- Sun Feb 01, 2004 9:20 pm
- Forum: Techniques and Tools
- Topic: Gecko fusible
- Replies: 23
- Views: 24759
Hi. We are all affected by the entry of cheap Chinese products. I'm a Filipino Chinese. Grew up in Philippines and our company has to compete with cheap China products in all product lines. Stained glass, sand relief casting, shower doors, wardrobe doors, glass sink. Tried a dozen approach to compet...
- Fri Jan 30, 2004 1:44 am
- Forum: Techniques and Tools
- Topic: source for hardware for sinks?
- Replies: 5
- Views: 7246
- Thu Jan 29, 2004 9:11 pm
- Forum: Techniques and Tools
- Topic: float sink schedule ok?
- Replies: 13
- Views: 12584
Thank you Yoduh 1/2 schedule is not for fusing. It is only enough to get the impression of sand and fiber paper aligator/snake skin pattern is made of rubber. The local shoe and sandal industry use it a lot. There are many patterns available. spread some sand on shelf mixture then press the pattern ...
- Wed Jan 28, 2004 9:42 pm
- Forum: Techniques and Tools
- Topic: float sink schedule ok?
- Replies: 13
- Views: 12584
Hello Yoduh Glass Sink Schedule for slumping on SS bowl, 6 pieces at a time I do this 2 to three cycles. Adjusting the glass to the center of the SS bowl on intervals 180 to 500 soak 0 200 to 950 soak 5 250 to 1145 soak 12 850 to 980 soak 45 180 to 800 soak 0 leave overnight This is what we use for ...
- Fri Jan 16, 2004 9:41 pm
- Forum: Techniques and Tools
- Topic: Tindicator problem
- Replies: 7
- Views: 8062
- Mon Jan 12, 2004 10:13 pm
- Forum: Techniques and Tools
- Topic: Happy Birthday WG!!
- Replies: 11
- Views: 11779
- Wed Nov 26, 2003 9:40 pm
- Forum: Techniques and Tools
- Topic: Enamel medium for waterslide decals
- Replies: 4
- Views: 6661
Hi. I did some experiment with enamel decals. The Medium has to be compatible with the covercoat. For screening enamel I use the polyester mesh 220 - 270. For screening covercoat I use the 55 to 80 mesh. Applying covercoat is the hardest part. It dries very quick and forms into web. I have to clean ...
- Sun Nov 23, 2003 10:40 pm
- Forum: Photos and Stuff
- Topic: first sand cast project
- Replies: 58
- Views: 64095
Brian Brian, One thing I did notice, even when I compacted this stuff and made a very simple pattern in it, the weight of the glass placed on top of the bentonite did eliminate much of the pattern. I'll keep you guys posted and let you know what happens on second attempt. Hi Dean. I also had the sa...
- Thu Oct 16, 2003 9:27 pm
- Forum: Techniques and Tools
- Topic: aluminum oxide
- Replies: 25
- Views: 27016
- Tue Oct 14, 2003 9:56 pm
- Forum: Techniques and Tools
- Topic: Craquelling and Marbling Lusters
- Replies: 8
- Views: 8260
- Mon Oct 13, 2003 10:12 pm
- Forum: Techniques and Tools
- Topic: Craquelling and Marbling Lusters
- Replies: 8
- Views: 8260
Craquelling and Marbling Lusters
Has anyone used this before?
http://www.amarinceramics.com/html/colour.html
under Lusters , Craquelling and Marbling solutions
Nelson
http://www.amarinceramics.com/html/colour.html
under Lusters , Craquelling and Marbling solutions
Nelson
- Wed Oct 01, 2003 8:58 pm
- Forum: Techniques and Tools
- Topic: Recommend 'thick glass' cutter
- Replies: 15
- Views: 14953
- Thu Sep 25, 2003 9:32 pm
- Forum: Techniques and Tools
- Topic: fire-polishing float after sandblasting
- Replies: 2
- Views: 6031
Hello Mark,
I did it while 1/2" green float glass is still flat. 1465 F. 18" diameter while flat.
http://community.webshots.com/user/yamatan
under glass sink
Nelson
I did it while 1/2" green float glass is still flat. 1465 F. 18" diameter while flat.
http://community.webshots.com/user/yamatan
under glass sink
Nelson
- Wed Sep 17, 2003 9:34 pm
- Forum: Techniques and Tools
- Topic: Finding Tin Side of Float Glass
- Replies: 17
- Views: 31008