Search found 8 matches
- Mon Jan 27, 2014 11:28 am
- Forum: Techniques and Tools
- Topic: kiln in unheated garage
- Replies: 9
- Views: 11795
Re: kiln in unheated garage
I agree who you most of the year. I live in Minnesota. My kiln was set at 75 and I turned it off to load it. Went in the house for less than a hour. The kiln had already dropped to 29. That is why I keep it at 75 until I can unload it.
- Sun Jan 26, 2014 6:01 pm
- Forum: Techniques and Tools
- Topic: kiln in unheated garage
- Replies: 9
- Views: 11795
Re: kiln in unheated garage
I have done some of my fuses with the starting temp of 20 in the kiln, going at 250/per. But I do make sure the temp goes down slowly all the way to 75 and holds until I will be able to get the glass out of the kiln.
- Wed Jan 01, 2014 9:48 pm
- Forum: Newcomer Forum
- Topic: Your favorite website for buying fusible glass and why?
- Replies: 13
- Views: 21337
Re: Your favorite website for buying fusible glass and why?
I use jringglass. They seem to have good prices.
- Sun May 26, 2013 4:41 pm
- Forum: Techniques and Tools
- Topic: Using a stainless steel ring and scrap clear glass
- Replies: 13
- Views: 13728
Re: Using a stainless steel ring and scrap clear glass
On Fusedglass.org under tools, there is a calculator you can use. It gives the weight that you need to use.
- Mon Apr 22, 2013 11:46 am
- Forum: Newcomer Forum
- Topic: magazines
- Replies: 7
- Views: 9064
Re: magazines
Glass Patterns Quarterly is a good magazine.
- Mon Jan 21, 2013 8:22 pm
- Forum: Newcomer Forum
- Topic: Schedule help and other questions.
- Replies: 15
- Views: 20915
Re: Schedule help and other questions.
Glass wants to be 6mm after a full fuse. If you use the thinner glass it will shrink up until it is 6mm thick. When you do jewelry making you are using many layers.
I don't see a bubble squeeze in your program. You might want to put one in if you do something very large.
I don't see a bubble squeeze in your program. You might want to put one in if you do something very large.
- Mon Jan 14, 2013 10:27 am
- Forum: Newcomer Forum
- Topic: Kiln recommendation?
- Replies: 5
- Views: 7166
Re: Kiln recommendation?
I like my Olympic kiln. I would get a square one, no matter which company you go with.
- Wed May 30, 2012 10:32 pm
- Forum: Kiln Casting
- Topic: HELP - Picking the right kiln
- Replies: 6
- Views: 9181
Re: HELP - Picking the right kiln
I have the Olympic GF314ETLC. I like it. Being a clam shell makes it easy to load, but it also opens from the top which is handy.