by S.TImmerman
Sun Nov 01, 2015 6:30 am
Forum: Kiln Casting
Topic: Plaster/silica mold improvements
Replies: 9
Views: 10316

Re: Plaster/silica mold improvements

Les, I agree that Zircar's a good place to look, but the problem isn't so much the mold as the release at prolonged temperatures of 2100F or thereabouts. MM6 might hold up, but I'm not sure I'd trust either kilnwash or most of the BN sprays I'd like to do some experimenting with paper clay under no...
by S.TImmerman
Mon Apr 20, 2015 3:31 am
Forum: Art, philosophy, and content
Topic: Silence
Replies: 26
Views: 31490

Re: Silence

I miss Brock too and and am now worried, I see he is no longer a "member" I hope its only temporary . Facebook groups Yes, there are some answers that are just plan scary; given to questions on Facebook's sites. Folks acting knowledgeable and/or authoritative - with very little experience ...
by S.TImmerman
Wed Feb 04, 2015 4:20 am
Forum: Kiln Casting
Topic: Plaster mold
Replies: 11
Views: 14429

Re: Plaster mold

I found a place that does aluminum casting and sells the investment. I have contacted them to buy some. I'll let you know!

http://www.avalon-castings.com/investme ... g/aluminum
by S.TImmerman
Wed Feb 04, 2015 3:46 am
Forum: Techniques and Tools
Topic: Vitrograph Kiln set up
Replies: 5
Views: 4623

Re: Vitrograph Kiln set up

I also use a vermiculite board, drilled a hole in it, I sat that on an old kiln shelf with a hole. I was worried about it cracking hence the kiln shelf under it. I also use a coller with my caladra so I can use taller pots.

Hope this is of some help

Shereen
by S.TImmerman
Mon Feb 02, 2015 10:50 pm
Forum: Kiln Casting
Topic: Plaster mold, 1st time questions
Replies: 13
Views: 15156

Re: Plaster mold, 1st time questions

I just love this board , I googled my question and such wonderful artists chime in. Thank you !
by S.TImmerman
Wed Jan 28, 2015 6:31 am
Forum: Techniques and Tools
Topic: Quenching glass
Replies: 22
Views: 15206

Re: Quenching glass

Hello neighbor ,

I bought an old SS MILK bucket and make Frit. Ann nye posted a video how she (well her husband) does it,

https://m.youtube.com/watch?v=p3mpWIv08lc

Enjoy the rain we've been getting!

Shereen
by S.TImmerman
Sun Jan 11, 2015 4:12 am
Forum: Newcomer Forum
Topic: Has anyone perfected opaque frit balls?
Replies: 11
Views: 12903

Re: Has anyone perfected opaque frit balls?

I use Coca-Cola to remove it.
by S.TImmerman
Sun Jan 11, 2015 4:10 am
Forum: Techniques and Tools
Topic: Where to buy ceramaguard
Replies: 4
Views: 4170

Re: Where to buy ceramaguard

Anyplace that sells Armstong ceiling tiles. If you need to buy more than you need i
I'll buy part of the box. My parents are in SF,

http://www.armstrong.com/commceilingsna ... -cZ1z141dp
by S.TImmerman
Sun Jan 11, 2015 4:06 am
Forum: Kiln Casting
Topic: Mold bits in my casting
Replies: 4
Views: 5210

Re: Mold bits in my casting

Cynthia, when are you going to take all your words of wisdom and have it typed up into a book? I'll bet most of its out there and you just need to organize it?

Sign me up please ..
by S.TImmerman
Thu Jan 08, 2015 8:58 am
Forum: Techniques and Tools
Topic: Making a mold of a bowl
Replies: 18
Views: 15739

Re: Making a mold of a bowl

Thank you Dana, The customer is still in Europe so as soon as they sail back I'll share this mold . I'll check bluefure contact info and call them about the size. I doubt my customer cares but it would be much cheaper to use a ready made mold. I'm still going to do the clay process as I love to lear...
by S.TImmerman
Mon Jan 05, 2015 8:18 am
Forum: Techniques and Tools
Topic: Making a mold of a bowl
Replies: 18
Views: 15739

Re: Making a mold of a bowl

Thank you all so much, what I've decided to do is carve the shape on a leather hard 14" round peice of clay. Fire it with vent holes. Pre fire a 1/4 in piece of glass and then use the mold with enamels/frit. Then slump it. Would screening enamels over the prepared mold be better than using frit...
by S.TImmerman
Sat Jan 03, 2015 5:17 am
Forum: Techniques and Tools
Topic: Making a mold of a bowl
Replies: 18
Views: 15739

Re: Making a mold of a bowl

Morginia , That's a great idea, I am going to change it a bit and they don't want clear. The colors are yellow/brown to go with green plates. Not my choice tho' however it's not as bad as the customer who wanted a full size ferret SG window a few years back for her bedroom window. Thank you very muc...
by S.TImmerman
Fri Jan 02, 2015 8:50 am
Forum: Techniques and Tools
Topic: Making a mold of a bowl
Replies: 18
Views: 15739

Making a mold of a bowl

Hello, Is it possible to make a mold of the inside of a bowl and utilize it? I was approached and asked if I could make 12 salad bowls just like this bowl which is made if some type of hard plastic. I do have a quart of silicon mold as well as ceramic mold and clay. Thank you Shereen My new year res...
by S.TImmerman
Fri Dec 19, 2014 3:26 am
Forum: Techniques and Tools
Topic: cloth "molds"
Replies: 9
Views: 7412

Re: cloth "molds"

I have some lava cloth and have used it make nice designs in glass. The ceramic lava cloth worked well for me, I wonder if it was different than the cloth you bought. I'll take a photo of the glass and post it.
Shereen
by S.TImmerman
Thu Dec 18, 2014 1:30 am
Forum: Techniques and Tools
Topic: Hanovia Gold
Replies: 11
Views: 8229

Re: Hanovia Gold

Thank you all, Yes I did mean .02 bottles - I wrote kathy and she replied very quickly - here are her instructions (I know how much the search tool has helped me in the past) The proper thinner for Bright Gold is the OH1 Essence $9.95/1/2 oz. It is made by the gold Factory and is the only thing I wo...
by S.TImmerman
Sun Dec 14, 2014 4:26 am
Forum: Techniques and Tools
Topic: Hanovia Gold
Replies: 11
Views: 8229

Hanovia Gold

Hello, I was given a dozen 2oz bottles of Hanovia gold and most of them need thinning- 2 are completely dry. They are (or were) sealed up and looking at the prices on them they are fairly old. I don't want to experiment putting something like clove oil if its not the correct thing. Does anyone know ...
by S.TImmerman
Thu Oct 09, 2014 4:37 am
Forum: Newcomer Forum
Topic: MAgazines
Replies: 5
Views: 5528

Re: MAgazines

Mike, If youre looking for magizines to learn techniques - one of the best deals are bullseye's online video education http://www.bullseyeglass.com/education/bullseye-kiln-glass-education-online.html Lots of free videos and you have access to all the past ones. Lastly, several months ago I bought 50...
by S.TImmerman
Sun Aug 24, 2014 6:03 pm
Forum: Techniques and Tools
Topic: Blaster Question
Replies: 12
Views: 9359

Re: Blaster Question

Jim, I too have the same standing cabinet, you might find this video helpful as he does some modifications of his cabinet. The issues I fixed right off was the poor lighting and the nozzle. Both of these are easily fixes. My next task is sealing areas where AO leaks a bit. Good luck https://m.youtub...
by S.TImmerman
Fri Jul 11, 2014 5:06 am
Forum: Techniques and Tools
Topic: 3d printers
Replies: 5
Views: 4206

3d printers

With 3d printers getting cheaper and larger Im very tempted to get one. What can a glass artist use one for? Besides making designs you can then make a mold with.

Thank you

Shereen
by S.TImmerman
Fri Jun 13, 2014 3:01 am
Forum: Techniques and Tools
Topic: Real gold
Replies: 5
Views: 4289

Re: Real gold

yes its all sealed -he sent me four boxes of it. Thank you for the link!

Id love to use it to draw on glass and fuse it!