Search found 9 matches

by debbie t
Wed Jul 27, 2016 9:55 pm
Forum: Kiln Casting
Topic: surface problem on casting
Replies: 5
Views: 13805

Re: surface problem on casting

I think I am not holding the melting temp long enough, did that and had success, I will also heat my molds to burn them out first. Thanks, Deb
by debbie t
Mon Jul 25, 2016 11:44 am
Forum: Kiln Casting
Topic: surface problem on casting
Replies: 5
Views: 13805

surface problem on casting

I have been experiencing some surface problems on my castings. has anyone had this problem before that can tell me why this is happening and how I can avoid it.
I use Bullseye frit with Ransome and Randloph casting material. Just switched to dust free bandust product.
surface problems
surface problems
small .jpg (100.84 KiB) Viewed 13805 times
Thank you Debbie
by debbie t
Tue Jan 20, 2015 7:09 pm
Forum: Kiln Casting
Topic: Removing Plaster from Mold
Replies: 16
Views: 26966

Re: Removing Plaster from Mold

Hi This is a lot to ask but can you go to e-bay and let me know which one looks like yours. I Saw them there but wouldn’t know which one it is. Thank you,
Best, Deb
by debbie t
Tue Jan 20, 2015 4:25 pm
Forum: Kiln Casting
Topic: Removing Plaster from Mold
Replies: 16
Views: 26966

Re: Removing Plaster from Mold

I was wondering which sonic pic did you purchase and how much did you pay for it. There are a few out there.
Thanks,
Debbie Tarsitano
by debbie t
Sat Jan 17, 2015 10:44 pm
Forum: Kiln Casting
Topic: Removing Plaster from Mold
Replies: 16
Views: 26966

Re: Removing Plaster from Mold

I am going to use the sonic pic will get one this week. I know what you mean, I have been schlepping water bottles for years. It is a simple solution to the problem of no water in the studio. I always feel like a pioneer on the prairie. I wish I lived closer to Corning 7 hours away. They have everyt...
by debbie t
Sat Jan 17, 2015 2:48 pm
Forum: Kiln Casting
Topic: Removing Plaster from Mold
Replies: 16
Views: 26966

Re: Removing Plaster from Mold

Hi , The dentil pic sounds like a good idea for the tight spaces. I tried an electric tooth brush, a friends idea, and believe it or not I was thinking of some of the abrasive tooth pastes they are making these days which have a grit in them but are gentle. I am going to try that next. The CRL seeme...
by debbie t
Fri Jan 16, 2015 8:16 pm
Forum: Kiln Casting
Topic: Removing Plaster from Mold
Replies: 16
Views: 26966

Re: Removing Plaster from Mold

Hi Jenna, Thanks for the help. I purchased the CRL today and will experiment with it. I will look into the primers and try them out too. Thank you for explaining how to use them. I wouldn’t have known where to start. When I have some results I will post them. It is a difficult process and it is true...
by debbie t
Fri Jan 16, 2015 11:18 am
Forum: Kiln Casting
Topic: Removing Plaster from Mold
Replies: 16
Views: 26966

Re: Removing Plaster from Mold

Hi Jenna, Thank you for your quick response. I was so happy to see your e-mail. I haven’t tried a kiln wash on my molds. I just place my Bullseye frit right into the clean plaster mold. I will try the kiln wash and CLR. How much kiln wash do you apply? The pieces I am making are very big over 30 inc...
by debbie t
Thu Jan 15, 2015 3:50 pm
Forum: Kiln Casting
Topic: Removing Plaster from Mold
Replies: 16
Views: 26966

Removing Plaster from Mold

Hi I have been casting for 5 years now. Today I am creating very large open face castings. Big pieces pose new problems. After removing most all of the plaster I am still left with surface plaster in some spots. Since the piece is very large it really does not fit into my available sandblaster. I ha...