Search found 124 matches
- Thu Jan 06, 2022 7:05 pm
- Forum: Newcomer Forum
- Topic: Frit colouring
- Replies: 3
- Views: 20578
Re: Frit colouring
Hi Jon. The questions about fusing stained glass have been frequent. If you enter "fusing stained glass" in the search box at the upper right of the screen, you may find the information you need. Information about float glass can be obtained the same way. Good luck.
- Tue Oct 19, 2021 9:58 am
- Forum: Techniques and Tools
- Topic: Fractures appeared!
- Replies: 11
- Views: 9549
Re: Fractures appeared!
I just looked at your website, Bonnie. Your work is outstanding! As long as you can make the glass work, I wouldn't change a thing.
- Sat Oct 02, 2021 12:03 pm
- Forum: Techniques and Tools
- Topic: The screw on running pliers.
- Replies: 20
- Views: 84601
Re: The screw on running pliers.
When you throw away the screw, just go ahead and discard the breaking pliers and buy Silberschnitt Running Pliers. They are pricey, but very easy to use and they swivel so you can slowly run a long cut not only from the end but along the length. The pliers are aluminum and the contact parts are high...
- Sun Aug 29, 2021 11:19 am
- Forum: Techniques and Tools
- Topic: Tiny Hole Saw Bits for a Dremel?
- Replies: 13
- Views: 26643
Re: Tiny Hole Saw Bits for a Dremel?
Not that I like Walmart but the quality is probably equal to many other Chinese items, and the price is right with the size starting at 6mm
https://www.walmart.com/ip/Diamond-Dril ... Method=wpa
https://www.walmart.com/ip/Diamond-Dril ... Method=wpa
- Thu Aug 19, 2021 10:12 am
- Forum: Techniques and Tools
- Topic: Tiny Hole Saw Bits for a Dremel?
- Replies: 13
- Views: 26643
Re: Tiny Hole Saw Bits for a Dremel?
That is interesting about Daniel. The last time I talked with him, he said he was no longer selling the bits and referred me to LAU. Guess he changed his mind. Happy drilling, Barry.
- Wed Aug 18, 2021 6:04 am
- Forum: Techniques and Tools
- Topic: Tiny Hole Saw Bits for a Dremel?
- Replies: 13
- Views: 26643
Re: Tiny Hole Saw Bits for a Dremel?
Daniel Lopaki is no longer selling diamond bits. I have not had good performance from LAU, at least not the small bits although the price is great. I tried the triple ripple bits in the 1mm size and so far I have drilled about 80 holes with the first bit. These are pricey bits, but the performance o...
- Wed Jan 20, 2021 12:05 pm
- Forum: Techniques and Tools
- Topic: Flat Lap
- Replies: 13
- Views: 29698
Re: Flat Lap
China is interesting. A couple of years ago I ordered some round pendant blanks and got oval ones. Last year I ordered some different metal findings and could only use about half due to permanent tarnishing and poor metal finishing. I just ordered several items which are supposed to ship within six ...
- Fri Dec 04, 2020 11:38 am
- Forum: Techniques and Tools
- Topic: Flat Lap
- Replies: 13
- Views: 29698
Re: Flat Lap
How about this...probably not the strongest attraction, but may be enough with all the surface area of the grinding disk. https://www.amazon.com/Rust-Oleum-247596-Magnetic-Primer-30/dp/B003ZW7XL4/ref=sr_1_1?dchild=1&gclid=EAIaIQobChMIton44NO07QIVF4-GCh27ggwjEAAYAiAAEgK5_fD_BwE&hvadid=1778070...
- Tue Nov 17, 2020 6:23 pm
- Forum: Photos and Stuff
- Topic: Re-worked Pendant
- Replies: 4
- Views: 30481
Re: Re-worked Pendant
Thanks, Don. I really admire your work. You are truly an artist!
- Fri Nov 13, 2020 3:24 pm
- Forum: Photos and Stuff
- Topic: Re-worked Pendant
- Replies: 4
- Views: 30481
Re: Re-worked Pendant
Thanks, Barry!!
- Fri Nov 13, 2020 11:46 am
- Forum: Photos and Stuff
- Topic: Re-worked Pendant
- Replies: 4
- Views: 30481
Re-worked Pendant
One of the things I like about fused glass is that it is sometimes possible to modify a piece years later. In this case, the attached pendants did not sell in their original configuration, so I enameled them and re-fired. I like them much better now, so maybe they will sell or not..., in any event I...
- Sat Nov 07, 2020 11:34 am
- Forum: Newcomer Forum
- Topic: Reading COE
- Replies: 2
- Views: 23830
Re: Reading COE
Hi Jan. When I read your question, I thought this should be easy to find with Google. It was not, because the actual measurement has been lost to the reduced reporting of 90, 96, 82. etc. I finally found the answer in an earlier post on the board: http://warmglass.com/phpBB3/viewtopic.php?t=41565 Lo...
- Thu Oct 15, 2020 8:41 pm
- Forum: Photos and Stuff
- Topic: Some Enamel Pendants
- Replies: 2
- Views: 27191
Re: Some Enamel Pendants
Hi Dana. I just put the standard glue-on bail on them like the one in this picture, but silver-plated. If I do anything more elaborate, it increases my price too much in the galleries and hurts my sales.
- Sun Oct 11, 2020 2:26 pm
- Forum: Photos and Stuff
- Topic: Some More Detailed Photos of the Enamels
- Replies: 3
- Views: 28133
Re: Some More Detailed Photos of the Enamels
Don, these are about 1.25 inches in diameter and are going to be pendants. The way I apply the enamels and the firing give a tremendous amount of detail to small pieces.
- Sat Oct 10, 2020 11:57 am
- Forum: Photos and Stuff
- Topic: Some More Detailed Photos of the Enamels
- Replies: 3
- Views: 28133
- Sat Oct 10, 2020 11:49 am
- Forum: Photos and Stuff
- Topic: Some Enamel Pendants
- Replies: 2
- Views: 27191
Some Enamel Pendants
Just opened the kiln after firing last night and thought I would share a quick photo of some of the enamel cabs. Not the best lighting and not the best focus, but, hey, it's Saturday morning and too much trouble to set-up the photo tent....
- Wed Sep 30, 2020 5:05 pm
- Forum: Newcomer Forum
- Topic: bubbles
- Replies: 2
- Views: 24637
Re: bubbles
Bullseye considers the micro bubbles a "feature" of the handmade glass aspect. I think they also consider the "runs" on the top surface the same, but those certainly cause me a lot of problems when trying to match the gradient in dichroic glass.
- Wed Sep 30, 2020 4:59 pm
- Forum: Techniques and Tools
- Topic: Concerning firing enamels
- Replies: 8
- Views: 18547
Re: Concerning firing enamels
Hi Havi. What a pain the virus is, even without being infected! I now understand and appreciate what you are trying to do. For the red ink, I am fairly certain adding frit will not help much, if any. However, if you can leave the red ink open for a while or transfer it to a larger, more open contain...
- Wed Sep 30, 2020 11:56 am
- Forum: Techniques and Tools
- Topic: Concerning firing enamels
- Replies: 8
- Views: 18547
Re: Concerning firing enamels
Hi Havi. You seem to have several potential problems, the first being that you do not have an accurate known temperature in one of your kilns, the one where you had the best results. You did not specify what enamels you are using either, and the range you fired of about 125 degrees between the firin...
- Thu Sep 17, 2020 3:41 pm
- Forum: Newcomer Forum
- Topic: kiln door gaskets-where to buy?
- Replies: 1
- Views: 12106
Re: kiln door gaskets-where to buy?
https://www.google.com/search?hl=en&tbm=isch&source=hp&biw=1135&bih=694&ei=J7tjX6m1A5fa-gSArKqwAw&q=kiln+gasket&oq=kiln+gasket&gs_lcp=CgNpbWcQAzoFCAAQsQM6AggAOgYIABAFEB46BggAEAgQHlCHEFijIWDHLWgAcAB4AIABoQGIAa0MkgEEMC4xMZgBAKABAaoBC2d3cy13aXotaW1nsAEA&sclient=img&...