Search found 4 matches
- Wed Nov 25, 2015 12:53 pm
- Forum: Newcomer Forum
- Topic: soap dish slumping
- Replies: 2
- Views: 6168
soap dish slumping
I am using a 4x6 piece of fibreboard 1/2 thick. It has a3/4 inch edge around it. So basically a rectangle with the center cut out. I slumped my glass but the bottom is curved causing the dish to rock. I am just placing the board on my kiln shelf. Is the rocking due to the fact my board is not high e...
- Fri Nov 06, 2015 5:16 pm
- Forum: Techniques and Tools
- Topic: sharp edges and small crack with a few bubbles
- Replies: 9
- Views: 13900
Re: sharp edges and small crack with a few bubbles
Glass is compatible, i used system 96 in a hotstart kiln only 13" wide..So my question is now..how do i fix this..ie firing schedule to remove sharp edges as i still want to slump it.
- Fri Nov 06, 2015 1:17 pm
- Forum: Techniques and Tools
- Topic: sharp edges and small crack with a few bubbles
- Replies: 9
- Views: 13900
Re: sharp edges and small crack with a few bubbles
Hi Judd
I have sent you an email with a better explanation, I hope
I have sent you an email with a better explanation, I hope
- Fri Nov 06, 2015 2:11 am
- Forum: Techniques and Tools
- Topic: sharp edges and small crack with a few bubbles
- Replies: 9
- Views: 13900
sharp edges and small crack with a few bubbles
so I hope this isn't too long a post. I fused a 10x10 piece first layer clear with black on either side and design in the middle. First fuse fine. Second fire was a clear sheet and dediced to do a bubble squeeze from Spectrum website. schedule 1st seg. 250 -250 hold30, 2nd 250-250 hold40, 3rd 200-12...